MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polygon Composites Polylube™ Fiber Series Epoxy Composite Bearings
Categories: Polymer; Thermoset; Epoxy; Epoxy, Encapsulating, Glass or Mineral Filled

Material Notes: Low friction coupled with high load carrying capacity are natural benefits. Teflon® superfilaments, which exhibit tensile strength twenty times greater than PTFE resins are integrated into the bearing surface. Polylube bearings resist cold flow and demonstrate impressive wear characteristics. Polygon's patented mechanical process of fiberglass filament weaving/winding results in structures of exceptional strength to support the bearing surface. A filament-wound fiberglass chemically bonded with epoxy, Polylube's structure is naturally concentric with no seam or overlap.

Information provided by Polygon Company. Teflon® is a registered trademark of DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.87 g/cc0.0676 lb/in³
Water Absorption 0.12 %0.12 %2 hours
 0.16 %0.16 %24 hours
 
Mechanical PropertiesMetricEnglishComments
Compressive Yield Strength 172 MPa25000 psiUnit Load Limit
Compressive Strength 379 MPa55000 psi
 
Thermal PropertiesMetricEnglishComments
CTE, linear 12.6 µm/m-°C
@Temperature 20.0 °C
7.00 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 0.259 - 0.331 W/m-K1.80 - 2.30 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 163 °C325 °FSpecial Formulation can go higher
Minimum Service Temperature, Air -196 °C-320 °F
 
Descriptive Properties
Max Velocity10 SFM

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polygon Composites Polylube® MRP Versatile high load, low friction composite bearings
Jushi E7 DR-386T Direct Roving - Epoxy Composite
Fibre Glast 1110 L Vinyl Ester Resin (Laminate Properties)
Overview of materials for Polyetheretherketone, Unreinforced
Overview of materials for Polyetheretherketone, Glass Fiber Filled

PPOLYG00 / 57161

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.