MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Domo TECHNYL® A 218 PA66, 33% glass fiber, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Standard viscosity, heat stabilized for injection molding. It is available in natural and black colors.

Benefits: This product offers all the primary properties of unreinforced polyamide 66. In addition, it has improved resistance to high temperature, and can be used for components which will withstand long-term temperature stresses.

Available in: Asia Pacific, Europe, Latin America and North America

Regulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applications.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³ISO 1183/A
Water Absorption 1.3 %
@Temperature 23.0 °C,
Time 86400 sec
1.3 %
@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Viscosity  20 cP
@Shear Rate 1000 1/s,
Temperature 290 °C
20 cP
@Shear Rate 1000 1/s,
Temperature 554 °F
 20.5 cP
@Shear Rate 1000 1/s,
Temperature 280 °C
20.5 cP
@Shear Rate 1000 1/s,
Temperature 536 °F
 60 cP
@Shear Rate 100 1/s,
Temperature 300 °C
60 cP
@Shear Rate 100 1/s,
Temperature 572 °F
 70 cP
@Shear Rate 100 1/s,
Temperature 290 °C
70 cP
@Shear Rate 100 1/s,
Temperature 554 °F
 100 cP
@Shear Rate 100 1/s,
Temperature 280 °C
100 cP
@Shear Rate 100 1/s,
Temperature 536 °F
 101 cP
@Shear Rate 10 1/s,
Temperature 300 °C
101 cP
@Shear Rate 10 1/s,
Temperature 572 °F
 105 cP
@Shear Rate 10 1/s,
Temperature 290 °C
105 cP
@Shear Rate 10 1/s,
Temperature 554 °F
 120 cP
@Shear Rate 10 1/s,
Temperature 280 °C
120 cP
@Shear Rate 10 1/s,
Temperature 536 °F
Linear Mold Shrinkage 0.010 cm/cm0.010 in/inIsotropy
Linear Mold Shrinkage, Flow 0.019 cm/cm0.019 in/in
Linear Mold Shrinkage, Transverse 0.019 cm/cm0.019 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 55.0 MPa7980 psiISO 527 Type 1A
Tensile Strength, Yield 90.0 MPa13100 psiISO 527 type 1 A
Tensile Stress at Strain  30.0 MPa
@Strain 1 %
4350 psi
@Strain 1 %
 58.0 MPa
@Strain 2 %
8410 psi
@Strain 2 %
 78.0 MPa
@Strain 3 %
11300 psi
@Strain 3 %
 85.0 MPa
@Strain 4 %
12300 psi
@Strain 4 %
Elongation at Break 30 %30 %ASTM D638
 50 %50 %ISO 527 Type 1A
Elongation at Yield 4.0 %4.0 %ISO 527 type 1 A
Tensile Modulus 3.00 GPa435 ksiISO 527 Type 1A
Flexural Strength 120 MPa17400 psiISO 178
 125 MPa18100 psiASTM D790
Flexural Modulus 3.00 GPa435 ksiISO 178
 3.30 GPa479 ksiASTM D790
Izod Impact, Notched 0.800 J/cm1.50 ft-lb/inASTM D256
Izod Impact, Unnotched NBNBASTM D256
Izod Impact, Notched (ISO) 4.00 kJ/m²1.90 ft-lb/in²ISO 180/1eA
Charpy Impact Unnotched NBNBISO 179/1eU
Charpy Impact, Notched 0.450 J/cm²2.14 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+15 ohm1.00e+15 ohmIEC 60093
Dielectric Constant 2.92.9IEC 60250
Dielectric Strength 25.0 kV/mm635 kV/inIEC 60243
Dissipation Factor 0.0300.030IEC 60250
Comparative Tracking Index 350 V350 VSolution B; IEC 60112
 600 V600 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
@Temperature 23.0 - 85.0 °C
38.9 µin/in-°F
@Temperature 73.4 - 185 °F
ISO 11359
Melting Point 263 °C505 °FISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 220 °C428 °FASTM D648
Flammability, UL94  V-2
@Thickness 1.60 mm
V-2
@Thickness 0.0630 in
1210
 V-2
@Thickness 3.20 mm
V-2
@Thickness 0.126 in
1210
Oxygen Index 26 %26 %ISO 4589
Glow Wire Flammability Index 650 °C
@Thickness 1.60 mm
1200 °F
@Thickness 0.0630 in
ISO 60695-2-12
 
Processing PropertiesMetricEnglishComments
Feed Temperature 265 - 275 °C509 - 527 °F
Mold Temperature 60.0 - 80.0 °C140 - 176 °F
Drying Temperature 80.0 °C176 °F
Moisture Content <= 0.20 %<= 0.20 %
 
Descriptive Properties
Compression Zone270-280°C
Mixing Zone280-290°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Domo TECHNYL® A 218 V30 BK 34 NG-K PA66, 33% glass fiber, DRY
Domo TECHNYL® A 218G2 V30 Black 34N PA66, 30% glass fiber, DRY
Domo Technyl® C216V30 30% Glass Filled Nylon 6
Domo TECHNYL® A 218G V30 PA66, 30% glass fiber, DRY
Domo TECHNYL® A 218G V33 Black 41N PA66, 33% glass fiber, DRY

PRHOD655 / 137886

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.