MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik Rohacell® 110EC-5 Electrically Conductive Grade Polymethacrylimide (PMI) Foam  (discontinued **)
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoset; Polymethacrylimide

Material Notes: ROHACELL® is produced by thermal expansion of a co-polymer sheet of methacrylic acid and methacrylonitrile. During the foaming process the copolymer sheet is converted to PMI - PolyMethacrylImide. Alcohol is used as a blowing agent, thus ROHACELL® contains no fluorinated carbon hydrates and is halogen free. It has a very homogeneous cell structure and isotropic properties.

Specific Notes for this Material: ROHACELL® EC (= Electrically Conductive) is a closed-cell rigid foam plastic based on PMI (polymethacrylimide) which does not contain any CFCs. ROHACELL® EC is a specially developed material for applications were electro conductivity is desirable. Any commonly used manufacturing technique, such as autoclave, press molding and resin infusionb can be applied. Thermoformability is another advantage of ROHACELL® EC.

Information provided by degussa.

Evonik Industries is the successor company to Degussa.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.110 g/cc0.00398 lb/in³DIN 53420, ISO 845, ASTM D 1622
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength 2.70 MPa392 psiDIN 53421, ISO 844, ASTM D 1621
Shear Strength 2.00 MPa290 psiDIN 53294, ASTM C 273
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 200 °C392 °FHeat Distortion Resistance; DIN 53424

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay A5000 FEP Fluoropolymer
Solvay AVIMID® RB Polyimide Composite
Solvay AVIMID® N Polyimide Composite
Saint-Gobain Norton® FEP Fluoropolymer Film
Dalau Dalcon 086 100% Virgin PTFE modified polymer

PROHA11 / 66316

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.