MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Rogers Arlon TC600 Thermally Conductive Ceramic Filled PTFE/Woven Fiberglass Laminate
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Microwave material for improved thermal management - for microwave printed circuit boards

  • Thermal Conductivity and Dielectric Constant Stability across Wide Temperatures
  • Very Low Loss Tangent provides higher Amplifier or Antenna Efficiency
  • Mechanically Strong; replaces brittle laminates that cannot withstand processing, impact or High G forces
  • Priced Affordably for Commercial Applications
  • High Peel Strength for Reliable Narrow Lines

Benefits:

  • Heat Dissipation and Management
  • Replace Ceramic in Some Applications
  • Improved Processing and Reliability
  • Large Panel Sizes for Multiple Circuit Layout for lowered Processing Costs

Typical Applications:

  • Power Amplifiers, Filters and Couplers
  • Microwave Combiner and Power Divider Boards in Avionics Applications
  • Small Footprint Antennas
  • Digital Audio Broadcasting (DAB) Antennas (Satellite Radio)
  • GPS & Hand-held RFID Reader Antennas

Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation.

Vendors: Arlon Materials for Electronics (MED) is a major manufacturer of specialty high performance laminate and prepreg materials for use in a wide variety of printed circuit board (PCB) applications and in several distinctive markets.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 2.90 g/cc0.105 lb/in³ASTM D792 Method A
Water Absorption 0.020 %0.020 %IPC TM-650 2.6.2.1
Outgassing - Total Mass Loss  0.00 %
@Pressure <=1.33e-10 MPa,
Temperature 125 °C
0.00 %
@Pressure <=1.93e-8 psi,
Temperature 257 °F
Water Vapor Recovered; NASA SP-R-0022A
 0.020 %
@Pressure <=1.33e-10 MPa,
Temperature 125 °C
0.020 %
@Pressure <=1.93e-8 psi,
Temperature 257 °F
NASA SP-R-0022A
Collected Volatile Condensable Material 0.00 %
@Pressure <=1.33e-10 MPa,
Temperature 125 °C
0.00 %
@Pressure <=1.93e-8 psi,
Temperature 257 °F
NASA SP-R-0022A
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 29.6 MPa4300 psiCross; IPC TM-650 2.4.18.3
 34.5 MPa5000 psiMachine; IPC TM-650 2.4.18.3
Modulus of Elasticity 1.93 GPa280 ksiIPC TM-650 2.4.18.3
Flexural Strength 64.1 MPa9300 psiCross; IPC TM-650 2.4.4
 66.2 MPa9600 psiMachine; IPC TM-650 2.4.4
Peel Strength 1.58 kN/m9.00 pliTo Copper (1 oz./35 micron); After Process Solutions; IPC TM-650 2.4.8
 1.75 kN/m10.0 pliTo Copper (1 oz./35 micron); After Thermal Stress; IPC TM-650 2.4.8
 1.75 kN/m10.0 pliTo Copper (1 oz./35 micron); At Elevated Temperatures; IPC TM-650 2.4.8.2
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.40e+14 ohm-cm2.40e+14 ohm-cmE24/125; IPC TM-650 2.5.17.1
 1.60e+15 ohm-cm1.60e+15 ohm-cmC96/35/90; IPC TM-650 2.5.17.1
Surface Resistance 9.00e+14 ohm9.00e+14 ohmE24/125; IPC TM-650 2.5.17.1
 3.10e+15 ohm3.10e+15 ohmC96/35/90; IPC TM-650 2.5.17.1
Dielectric Constant  6.15
@Frequency 1e+10 Hz
6.15
@Frequency 1e+10 Hz
may vary by thickness; IPC TM-650 2.5.5.5
 6.15
@Frequency 1.80e+6 Hz
6.15
@Frequency 1.80e+6 Hz
may vary by thickness; Resonant Cavity
Dielectric Strength 33.5 kV/mm850 kV/inIPC TM-650 2.5.6.2
Dielectric Breakdown 62000 V62000 VIPC TM-650 2.5.6
Dissipation Factor  0.0017
@Frequency 1.80e+9 Hz
0.0017
@Frequency 1.80e+9 Hz
may vary by thickness; Resonant Cavity
 0.0020
@Frequency 1e+10 Hz
0.0020
@Frequency 1e+10 Hz
may vary by thickness; IPC TM-650 2.5.5.5
Arc Resistance >= 240 sec>= 240 secIPC TM-650 2.5.1
 
Thermal PropertiesMetricEnglishComments
CTE, linear 9.00 µm/m-°C
@Temperature 50.0 - 150 °C
5.00 µin/in-°F
@Temperature 122 - 302 °F
IPC TM-650 2.4.41
CTE, linear, Transverse to Flow 35.0 µm/m-°C
@Temperature 50.0 - 150 °C
19.4 µin/in-°F
@Temperature 122 - 302 °F
z direction; IPC TM-650 2.4.24
Thermal Conductivity 1.10 W/m-K7.63 BTU-in/hr-ft²-°Fz-axis; ASTM E1461
 1.40 W/m-K9.72 BTU-in/hr-ft²-°Fx, y; ASTM E1461
Decomposition Temperature 512 °C954 °FInitial; IPC TM-650 2.4.24.6
 572 °C1060 °F5 percent; IPC TM-650 2.4.24.6
Flammability, UL94 V-0V-0
 
Descriptive Properties
IPC Delamination - T260 (minutes)> 60IPC TM-650 2.4.24.1
IPC Delamination - T288 (minutes)> 60IPC TM-650 2.4.24.1
IPC Delamination - T300 (minutes)> 60IPC TM-650 2.4.24.1
Temperature Coefficient of Dielectric (ppm/°C)-75IPC TM-650 2.5.5.5; at 10 GHz (-40 - 150°C)
Z-Axis Expansion (%)1.5IPC TM-650 2.4.24 (50-260°C)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Epoxy Technology EPO-TEK® H20E-PFC Electrically Conductive, Silver Epoxy
Mitsubishi Chemical Advanced Materials Fluorosint™ 135 PTFE and PPS Blend, with Proprietary Lubrication Fillers
Mitsubishi Chemical Advanced Materials Fluorosint™ 500 PTFE, synthetic mica-filled PTFE, compression molded
Mitsubishi Chemical Advanced Materials Fluorosint™ HPV PTFE Mica-filled
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded

PARLM9868 / 149021

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.