MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Titanium Grade 7
Categories: Metal; Nonferrous Metal; Titanium Alloy; Unalloyed/Modified Titanium

Material Notes: Titanium Grade 11 is identical (0.2% Pd) except for impurity limits. Pd added for corrosion resistance, very effective for improving crevice corrosion at elevated temperatures and where in contact with mildly reducing or variable oxidizing-reducing media. Properties are very similar to Ti Grade 2 because addition of small amount of Pd does not significantly change microstructure.

Applications: Chemical processing and storage - containers, heat exchangers, ducting, pumps, valves, fittings and auxiliary equipment.

Forms typically available: billet, bar, plate, sheet, strip, rod, wire, extrusions, tubing.

Titanium Grades 1,2,3,4,7,11,and 12 are all considered unalloyed and have similar mechanical properties.

Key Words: ASTM Grade 7; UNS R52400, CP titanium, C.P. titanium alloy
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 4.50 g/cc0.163 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 200200annealed
Hardness, Knoop 222222Estimated from Brinell.
Hardness, Rockwell B 7575annealed
Hardness, Rockwell C 1111Converted from Brinell hardness. Value below normal HRC range, for comparison purposes only.
Hardness, Vickers 209209Estimated from Brinell.
Tensile Strength, Ultimate 344 MPa49900 psi
Tensile Strength, Yield 275 - 410 MPa39900 - 59500 psi
Elongation at Break 20 %20 %
Tensile Modulus 105 GPa15200 ksi
Compressive Modulus 110 GPa16000 ksi
Poissons Ratio 0.370.37
Shear Modulus 45.0 GPa6530 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000550 ohm-cm0.0000550 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 325 J/g140 BTU/lbHigh Purity Ti.
CTE, linear  8.60 µm/m-°C
@Temperature 0.000 - 100 °C
4.78 µin/in-°F
@Temperature 32.0 - 212 °F
 9.20 µm/m-°C
@Temperature 0.000 - 315 °C
5.11 µin/in-°F
@Temperature 32.0 - 599 °F
average
 9.70 µm/m-°C
@Temperature 0.000 - 540 °C
5.39 µin/in-°F
@Temperature 32.0 - 1000 °F
perpendicular to the c-axis
Specific Heat Capacity  0.523 J/g-°C
@Temperature 23.0 °C
0.125 BTU/lb-°F
@Temperature 73.4 °F
 0.670 J/g-°C
@Temperature 540 °C
0.160 BTU/lb-°F
@Temperature 1000 °F
Thermal Conductivity 16.4 W/m-K114 BTU-in/hr-ft²-°Fannealed
Melting Point <= 1665 °C<= 3029 °F
Liquidus 1665 °C3029 °F
Maximum Service Temperature, Air 425 °C797 °FContinuous use
 540 °C1000 °FIntermittent Use
Beta Transus 913 °C1680 °F
 
Optical PropertiesMetricEnglishComments
Emissivity (0-1) 0.30
@Temperature 710 °C
0.30
@Temperature 1310 °F
High purity Ti
Reflection Coefficient, Visible (0-1) 0.560.56High purity Ti; visible light.
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.10 %<= 0.10 %
Hydrogen, H <= 0.015 %<= 0.015 %
Iron, Fe <= 0.30 %<= 0.30 %
Nitrogen, N <= 0.030 %<= 0.030 %
Other, each <= 0.050 %<= 0.050 %
Other, total <= 0.30 %<= 0.30 %
Oxygen, O <= 0.25 %<= 0.25 %
Palladium, Pd 0.12 - 0.25 %0.12 - 0.25 %
Titanium, Ti 99 - 99.8 %99 - 99.8 %As remainder

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Titanium Grade 2
Titanium Grade 4
Titanium Grade 3
Titanium Grade 1
Titanium Grade 11

MTU070 / 14265

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.