MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Huntsman IROGRAN® A 80 H 4826 TPU-Polyester
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Introduction: IROGRAN A 80 H 4826 is a thermoplastic polyester-polyurethane for injection molding applications. Additional characteristics of this product are excellent mechanical properties and high tear strength.

Performance Features:

  • high wear resistance
  • medium crystallinity
  • low hardness
  • increase of productivity
  • easy coloring
Applications: For the production of general injection molding, screens, wheels and rollers, buffers, shoe heal lifts

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³Injection molded parts; ISO 2781
Linear Mold Shrinkage 0.0085 cm/cm0.0085 in/in
Melt Index of Compound 20 g/10 min
@Load 21.6 kg,
Temperature 190 °C
20 g/10 min
@Load 47.6 lb,
Temperature 374 °F
MVR, [cm3/10 min]
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8181Injection molded parts; ISO 868
Hardness, Shore D 3030Injection molded parts; ISO 868
Tensile Strength at Break 39.3 MPa5700 psiInjection molded parts; ISO 37
Elongation at Break 600 %600 %Injection molded parts; ISO 37
100% Modulus 5.00 MPa
@Strain 100 %
725 psi
@Strain 100 %
Injection molded parts; ISO 37
300% Modulus 10.1 MPa
@Strain 300 %
1460 psi
@Strain 300 %
Injection molded parts; ISO 37
Rebound 44 %44 %Bayshore
Tear Strength 96.4 kN/m550 pliInjection molded parts; ISO 34B
Abrasion 2525mm3, Injection molded; ISO 4649
Compression Set  20 %
@Temperature 22.8 °C,
Time 252000 sec
20 %
@Temperature 73.0 °F,
Time 70.0 hour
Injection molded; ISO 815
 35 %
@Temperature 70.0 °C,
Time 86400 sec
35 %
@Temperature 158 °F,
Time 24.0 hour
Injection molded; ISO 815
 
Thermal PropertiesMetricEnglishComments
Melting Point 165 - 173 °C329 - 343 °F0.025" extruded film,
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 195 °C383 °F
Zone 1 190 °C374 °F
Zone 2 205 °C401 °F
Zone 3 195 °C383 °F
Drying Temperature 85.0 °C185 °F
Dry Time 2.00 hour2.00 hour
Dew Point -30.0 °C-22.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Huntsman IROGRAN® A 78 P 4766 NM Ether-Based TPU-For Cable Industry
Lubrizol ESTANE® T5384 Ether Based Thermoplastic Polyurethane
Huntsman IROGRAN® A 75 P 4665N TPU-Polyether
Huntsman IROGRAN® A 80 P 4699L Ether-Based TPU-For Cable Industry
Huntsman IROGRAN® A 80 P 5039 TPU-Polyether

PHUQ091 / 159464

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.