MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Huntsman IROGRAN® A 80 P 4699L Ether-Based TPU-For Cable Industry
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Ether Grade

Material Notes: Introduction: IROGRAN A 80 P 4699 L is a high performance polyether based thermoplastic polyurethane intended for extrusion and injection mold applications. IROGRAN A 80 P 4699 L is part of the HUNTSMAN extrusion / injection mold product range.

Performance Features:

  • Good melt flow
  • Low adhesion surface
  • High flexibility
  • Good processability
  • Soft

Information provided by Huntsman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.09 g/cc1.09 g/ccASTM D792
Linear Mold Shrinkage 0.0011 cm/cm0.0011 in/in
Melt Index of Compound 140 g/10 min
@Load 10.0 kg,
Temperature 190 °C
140 g/10 min
@Load 22.0 lb,
Temperature 374 °F
cm3/10 min
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8080ASTM D2240
Tensile Strength at Break 30.0 MPa4350 psiDIN 53504
Elongation at Break 670 %670 %DIN 53504
100% Modulus 5.70 MPa
@Strain 100 %
827 psi
@Strain 100 %
DIN 53504
300% Modulus 8.40 MPa
@Strain 300 %
1220 psi
@Strain 300 %
DIN 53504
Rebound 46 %46 %Bayshore; ASTM D2632
Tear Strength 76.0 kN/m434 pliDIN 5315
Abrasion 5050mm3; DIN 53516
Compression Set  24 %
@Temperature 23.0 °C,
Time 79200 sec
24 %
@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395
 46 %
@Temperature 70.0 °C,
Time 79200 sec
46 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D395
 
Processing PropertiesMetricEnglishComments
Feed Temperature 175 °C347 °FExtrusion
Front Barrel Temperature 180 °C356 °FExtrusion
Adapter Temperature 180 °C356 °FExtrusion
Die Temperature 175 °C347 °FExtrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Huntsman IROGRAN® A 78 P 4766 NM Ether-Based TPU-For Cable Industry
Huntsman IROGRAN® A 75 P 4665N TPU-Polyether
Huntsman IROGRAN® A 80 P 5039 TPU-Polyether
Huntsman IROGRAN® A 85 P 4441 TPU-Polyether
Huntsman IROGRAN® A 85 P 4666 Ether-Based TPU-For Cable Industry

PHU9943 / 150403

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.