MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Braskem BS600 HDPE Blow Molding Polyethylene Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: BS600 resin is a high-density polyethylene (HDPE), bimodal copolymer offering an outstanding combination of impact resistance and environmental stress crack resistance (ESCR). It is thus recommended for the production of containers, flasks, and bottles up to 30 liters for the transport of dangerous goods. Its other applications include bottles for agrochemicals and flasks for concentrated detergents and chemical products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.954 g/cc0.0345 lb/in³ASTM-D792
ESCR 100% Igepal® 520 hour
@Thickness 2.00 mm,
Temperature 50.0 °C
520 hour
@Thickness 0.0787 in,
Temperature 122 °F
0.3 mm notched-plaques; ASTM-D1693
ESCR 10% Igepal® 198 hour
@Thickness 2.00 mm,
Temperature 50.0 °C
198 hour
@Thickness 0.0787 in,
Temperature 122 °F
0.3 mm notched-plaques; ASTM-D1693
Melt Flow  0.70 g/10 min
@Load 5.00 kg,
Temperature 190 °C
0.70 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ASTM-D1238
 17 g/10 min
@Load 21.6 kg,
Temperature 190 °C
17 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ASTM-D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6666ASTM-D2240
Tensile Strength at Break 32.0 MPa4640 psiASTM-D638
Tensile Strength, Yield 30.0 MPa4350 psiASTM-D638
Flexural Modulus, 1% Secant 1030 MPa149000 psiASTM-D790
Izod Impact, Notched 1.54 J/cm2.89 ft-lb/inASTM-D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 71.0 °C160 °FASTM-D648
Vicat Softening Point 128 °C
@Load 1.02 kg
262 °F
@Load 2.25 lb
ASTM-D1525

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Braskem GF4950HS HDPE Blow Molding Polyethylene Copolymer
Chevron Phillips Marlex® HXM 50100 Extra high molecular weight hexene copolymer
Braskem BS002HS HDPE Blow Molding Polyethylene Copolymer
Braskem GF5250 HDPE Blow Molding Polyethylene Copolymer
Braskem HB0454 HDPE Blow Molding Polyethylene Copolymer

PBRAS881 / 106727

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.