MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BCC Products BC 8782 Urethane Casting
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: BC 8782 produces a high impact rigid 82 Shore D material that is commonly used to make clear or tinted castings of all kinds. When used at room temperature castings 1/8" thick or larger can be readily cast. Castings that are less than 1/8" thick generally require a mild post-cure. This system is not recommended for use with tin cure silicones.

Information provided by BCC Products, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.04 g/cc1.04 g/cc
Brookfield Viscosity 550 cP550 cPPart B
 650 cP650 cPMixed
 600 cP
@Temperature 25.0 °C
600 cP
@Temperature 77.0 °F
Part A
Linear Mold Shrinkage 0.00030 cm/cm0.00030 in/inASTM D2566
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 82
@Temperature 23.9 °C
82
@Temperature 75.0 °F
ASTM D2240-68
Tensile Strength, Ultimate 32.4 MPa4700 psiASTM D638-82
Elongation at Break 7.0 - 10 %7.0 - 10 %ASTM D790
Tensile Modulus >= 0.621 GPa>= 90.0 ksi5% strain; ASTM D790
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 73.9 °C165 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  360 - 480 min
@Temperature 24.0 °C
6.00 - 8.00 hour
@Temperature 75.2 °F
demold time
 7200 - 10080 min
@Temperature 24.0 °C
120 - 168.0 hour
@Temperature 75.2 °F
full cure
Pot Life 12 - 14 min
@Temperature 24.0 °C
12 - 14 min
@Temperature 75.2 °F
mass dependent
 
Descriptive Properties
Mix Ratio100:85 by weight, 100:88 by volume, resin/harder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BCC Products BC 8165 Urethane Casting
BCC Products Proto-Kast BC 8163 Urethane Casting
BCC Products BC 8405 Urethane Casting
BCC Products BC 8160 Urethane Casting
BCC Products DP-11-90 Urethane Casting

PBCC056 / 107283

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.