MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BCC Products BC 8165 Urethane Casting
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: BC 8165 is a low viscosity, rapid setting, rigid urethane compound. This system will cure quickly to a hard, tough, impact resistant casting. BC 8165 is non-sensitive to moisture after cure and will readily bond to itself if stage pours are required. BC 8165 is recommended for thin wall model and prototype applications where a "thermoplastic feel" is desired. The heat resistance for BC8165 is 135°F, a heat resistance of 150°F can be achieved by post cure at 150°F for about 2 hours.

Information provided by BCC Products, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.07 g/cc1.07 g/cc
Brookfield Viscosity 640 cP640 cPPart B
 36 cP
@Temperature 23.9 °C
36 cP
@Temperature 75.0 °F
Part A
 230 cP
@Temperature 23.9 °C
230 cP
@Temperature 75.0 °F
Mixed
Linear Mold Shrinkage 0.0010 cm/cm0.0010 in/inASTM D2566
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 81 - 85
@Temperature 23.9 °C
81 - 85
@Temperature 75.0 °F
Tensile Strength, Ultimate 40.0 MPa5800 psiASTM D638
Elongation at Break 2.4 %2.4 %ASTM D638
Flexural Strength 52.7 MPa7650 psiASTM D790
Flexural Modulus 1.45 GPa210 ksiASTM D790
 
Processing PropertiesMetricEnglishComments
Cure Time  60.0 - 120 min
@Temperature 24.0 °C
1.00 - 2.00 hour
@Temperature 75.2 °F
demold time
 10080 min
@Temperature 24.0 °C
168.0 hour
@Temperature 75.2 °F
full cure
Pot Life 8.0 - 10 min
@Temperature 24.0 °C
8.0 - 10 min
@Temperature 75.2 °F
1 lb. mass
 
Descriptive Properties
Mix Ratio100:80 by weight, 100:87 by volume, resin/harder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BCC Products BC 8405 Urethane Casting
BCC Products BC 8400 Urethane Casting
BCC Products DP-11-90 Urethane Casting
BCC Products Kwik Kast BC 8001 Urethane Casting
BCC Products Kwik Kast BC 8002 Urethane Casting

PBCC053 / 107280

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.