MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 285 D SI 2 Nylon 6/12 (PA), Carbon Fiber - Silicone Lubricated
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 612 (PA612); Nylon 612, Carbon Fiber Filler

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D 792
Filler Content 30 %30 %Primary Additive
Linear Mold Shrinkage 0.00050 - 0.0030 cm/cm
@Thickness 3.17 mm
0.00050 - 0.0030 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 207 MPa30000 psiASTM D 638
Elongation at Break 1.5 - 2.5 %1.5 - 2.5 %ASTM D 638
Tensile Modulus 19.7 GPa2850 ksiASTM D 638
Flexural Strength 303 MPa44000 psiASTM D 790
Flexural Modulus 17.6 GPa2550 ksiASTM D 790
Izod Impact, Notched 1.01 J/cm
@Thickness 3.17 mm
1.90 ft-lb/in
@Thickness 0.125 in
D 256
Izod Impact, Unnotched 8.01 J/cm
@Thickness 3.17 mm
15.0 ft-lb/in
@Thickness 0.125 in
ASTM D4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 0.10 - 10 ohm-cm0.10 - 10 ohm-cmASTM D 257
Surface Resistivity per Square 100 ohm - 1e+05100 ohm - 1e+05ASTM D 257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 216 °C420 °FASTM D 648
Flammability, UL94 HB
@Thickness 1.59 mm
HB
@Thickness 0.0625 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 249 - 285 °C480 - 545 °F
Mold Temperature 60.0 - 93.3 °C140 - 200 °F
Drying Temperature 79.4 °C175 °F
Dry Time 4 hour4 hour
Moisture Content 0.20 %0.20 %
Dew Point -17.8 °C0.000 °F
Injection Pressure 68.9 - 124 MPa10000 - 18000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 2286 HF TFE 15  Polyetheretherketone (PEEK) Carbon Fiber 35% - PTFE 15% - High Flow
RTP Company RTP 283 D TFE 15 Nylon 6/12 (PA), Carbon Fiber - PTFE Lubricated
RTP Company RTP 2799S X 89622 C  Styrenic Thermoplastic Elastomer (TES) Thermally Conductive - Electrically Conductive - SEBS
RTP Company RTP 2585 HEC Polycarbonate/ABS Alloy (PC/ABS); Nickel-Coated Carbon Fiber - Electrically Conductive - EMI/RFI Shielding
RTP Company RTP 2799 S X 91655 BLACK Saturated Styrenic Block Copolymer

PQZWA1234 / 90700

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.