MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Inno-Comp INNOPOL® CS 2-4630 GFR Flame Retarded Polypropylene Block-Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Flame Retardant

Material Notes: INNOPOL® CS 2-4630 GFR is a flame retarded polypropylene block-copolymer compound. This grade is available in nature and custom colored form.

INNOPOL® CS 2-4630 GFR is recommended for producing injection molded products, where the required properties are excellent flame retardancy (V0) besides balanced physical properties.

All information provided by INNO-COMP.

Key Words: PP-B
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.950 g/cc
@Temperature 23.0 °C
0.0343 lb/in³
@Temperature 73.4 °F
ISO 1183
Melt Flow 6.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
6.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 23.0 MPa3340 psi50 mm/min; ISO 527-1,-2
Elongation at Yield 5.0 %5.0 %50 mm/min; ISO 527-1,-2
Tensile Modulus 1.30 GPa189 ksi2 mm/min; ISO 527-1,-2
Flexural Modulus 1.45 GPa210 ksi2 mm/min; ISO 178
Izod Impact, Notched (ISO)  3.50 kJ/m²
@Temperature -20.0 °C
1.67 ft-lb/in²
@Temperature -4.00 °F
ISO 179/1eA
 5.00 kJ/m²
@Temperature 23.0 °C
2.38 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C194 °FISO 75-1,-2
Flammability, UL94 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
FMVSS 302
 
Descriptive Properties
Automotive MaterialsPassFMVSS 302
ColorGrey

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese SO.F.TER Polifor® 5220/V0-EP Mineral Filled Self Extinguishing Polypropylene, Flame Resistant
LATI Latene® 7H2W T-V0 PP Homopolymer, Mineral Reinforced, Heat Stabilized, Flame Retardant
LyondellBasell Pro-fax™ SG899 Polypropylene Copolymer
LyondellBasell Astryn BA905-74 Polypropylene Copolymer, Flame Retardant
Celanese SO.F.TER Talcoprene® C340TC Talc-Reinforced Polypropylene

PINNO044 / 82705

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.