MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Avient Trilliant™ HC FPO PPC-10G Natural PP Copolymer with 10% Glass Fabric  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 10% Glass Fiber Filler

Material Notes: The Trilliant® HC specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead of the competition. When specified, Trilliant HC compounds may incorporate agency rated materials that meet USP Class VI, FDA or ISO 10993 testing requirements.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.958 g/cc0.958 g/ccASTM D792
Filler Content 10 %10 %Glass Fabric
Linear Mold Shrinkage, Flow 0.0020 - 0.0050 cm/cm0.0020 - 0.0050 in/inASTM D955
Melt Flow 3.0 - 12 g/10 min3.0 - 12 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 39.3 MPa5700 psiType I, 51 mm/min; ASTM D638
Elongation at Break 12 %12 %Type I, 51 mm/min; ASTM D638
Flexural Strength 44.1 MPa6400 psiASTM D790
Flexural Modulus 1.93 GPa280 ksiASTM D790
Izod Impact, Notched 0.854 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
1.60 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 151 °C
@Thickness 3.18 mm
304 °F
@Thickness 0.125 in
Annealed; ASTM D648
 
Descriptive Properties
AppearanceNatural Color
FeaturesCopolymer
 General Purpose
 Impact Modified
FormsPellets
Generic NamePolypropylene Copolymer
Processing MethodInjection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesAutomotive Applications
 Construction Applications
 Consumer Applications
 General Purpose
 Industrial Applications

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 199 X 138766 Z EG Polypropylene (PP); Permanently Static Dissipative - ESD Protection - FDA Compliant Ingredients - Extrusion Grade
NIZHNEKAMSKNEFTEKHIM PP 1500J (T30G) Propylene Homopolymer
Ineos H03BLME Polypropylene Homopolymer
Braskem H521 Homopolymer Polypropylene
Braskem H 503 Raffia Extrusion & Fiber Extrusion Polypropylene Homopolymer

PH1PN9513 / 103349

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.