System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Cellulose Acetate Butyrate (CAB) Film
Categories:
Polymer
;
Film
;
Thermoplastic
;
Cellulosic
Material Notes:
Ultra Clear cellulose acetate butyrate film, low shrinkage, additive free, pinhole free; can be formulated with additives. Information typical of products used for flexible electronics.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Thickness
13.0
-
76.0
microns
0.512
-
2.99
mil
Electrical Properties
Metric
English
Comments
Dielectric Strength
88.0
kV/mm
2240
kV/in
Thermal Properties
Metric
English
Comments
Melting Point
235
°C
455
°F
Shrinkage
1.0 %
1.0 %
Optical Properties
Metric
English
Comments
Haze
0.83 %
0.83 %
Gloss
138 %
138 %
Transmission, Visible
94.1 %
94.1 %
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Cotronics Duralco™ 125 450°F Stress Free, Silver Filled Epoxy, Thermally Conductive
AGC F-Clean® GR
Evonik Trogamid® CX9701 Transparent Nylon
Mitsui TPX® DX820 Methylpentene Copolymer
Dow HV 1520/40
PFLEXSM03 / 179519
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.