MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient Bergamid™ A700 G25 U-SO Polyamide 66 (Nylon 66)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes:

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.38 g/cc0.0499 lb/in³±0.02 g/cm³; DIN 53479
Filler Content 25 %25 %Glass Fiber Reinforcement
Ash 25 %25 %ISO 3451
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 160 MPa
@Temperature 23.0 °C
23200 psi
@Temperature 73.4 °F
ISO 527-2/5
Elongation at Break 3.0 %
@Temperature 23.0 °C
3.0 %
@Temperature 73.4 °F
ISO 527-2/5
Tensile Modulus 8.50 GPa
@Temperature 23.0 °C
1230 ksi
@Temperature 73.4 °F
ISO 527-2/1
Charpy Impact Unnotched  6.00 J/cm²
@Temperature -30.0 °C
28.6 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 6.50 J/cm²
@Temperature 23.0 °C
30.9 ft-lb/in²
@Temperature 73.4 °F
Type 1; ISO 179/1eU
Charpy Impact, Notched  0.900 J/cm²
@Temperature -30.0 °C
4.28 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 1.20 J/cm²
@Temperature 23.0 °C
5.71 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 60093
Dielectric Constant 3.5
@Frequency 1e+6 Hz
3.5
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 80.0 kV/mm2030 kV/inIEC 60243-1
Dissipation Factor 0.015
@Frequency 1e+6 Hz
0.015
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 400 V400 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 261 °C502 °FISO 3146
Maximum Service Temperature, Air 120 °C248 °FContinuous (GTP 50% Tensile); IEC 60216
 220 °C428 °FShort Time; IEC 60216
Deflection Temperature at 0.46 MPa (66 psi) 250 °C482 °FUnannealed; ISO 75-2/B
Flammability, UL94 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
ALL; Internal Method
Glow Wire Ignition Temperature 960 °C
@Thickness 3.00 mm
1760 °F
@Thickness 0.118 in
0.8 mm wire; Ignition Temperature; IEC 60695-2-13
 
Descriptive Properties
AdditiveHeat Stabilizer
FeaturesFlame Retardant
 Halogen Free
 Heat Stabilized
FormsPellets
Generic MaterialNylon 66
Generic NamePolyamide 66 (Nylon 66)
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
RoHS ComplianceRoHS Compliant

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Bergamid™ A700 G25 HW UF Polyamide 66 (Nylon 66)
Celanese Zytel® ST801 NC010A PA66-HI
Avient Bergamid™ A700 Polyamide 66 (Nylon 66), Conditioned
Avient Bergamid™ A700 G20 HW UF Polyamide 66 (Nylon 66)
Avient Bergamid™ A700 G15 HW UF Polyamide 66 (Nylon 66)

PH0POL1131 / 145700

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.