MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient Bergamid™ A700 G20 HW UF Polyamide 66 (Nylon 66)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes:

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.34 g/cc0.0484 lb/in³±0.03 g/cm³; DIN 53479
Filler Content 20 %20 %Glass Fiber Reinforcement
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 115 MPa
@Temperature 23.0 °C
16700 psi
@Temperature 73.4 °F
ISO 527-2/5
Elongation at Break 3.0 %
@Temperature 23.0 °C
3.0 %
@Temperature 73.4 °F
ISO 527-2/5
Tensile Modulus 8.00 GPa
@Temperature 23.0 °C
1160 ksi
@Temperature 73.4 °F
ISO 527-2/1
Charpy Impact Unnotched 4.50 J/cm²
@Temperature 23.0 °C
21.4 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 0.550 J/cm²
@Temperature 23.0 °C
2.62 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
Melting Point 261 °C502 °FISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 250 °C482 °FUnannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 240 °C464 °FUnannealed; ISO 75-2/A
Vicat Softening Point 245 °C473 °FISO 306/A50
 245 °C473 °FISO 306/B50
UL RTI, Electrical  125 °C
@Thickness 0.750 mm
257 °F
@Thickness 0.0295 in
UL 746
 125 °C
@Thickness 1.50 mm
257 °F
@Thickness 0.0591 in
UL 746
 125 °C
@Thickness 3.00 mm
257 °F
@Thickness 0.118 in
UL 746
UL RTI, Mechanical with Impact  100 °C
@Thickness 0.750 mm
212 °F
@Thickness 0.0295 in
UL 746
 110 °C
@Thickness 1.50 mm
230 °F
@Thickness 0.0591 in
UL 746
 120 °C
@Thickness 3.00 mm
248 °F
@Thickness 0.118 in
UL 746
UL RTI, Mechanical without Impact  105 °C
@Thickness 0.750 mm
221 °F
@Thickness 0.0295 in
UL 746
 115 °C
@Thickness 1.50 mm
239 °F
@Thickness 0.0591 in
UL 746
 125 °C
@Thickness 3.00 mm
257 °F
@Thickness 0.118 in
UL 746
Flammability, UL94  V-0
@Thickness 0.400 mm
V-0
@Thickness 0.0157 in
ALL; UL 94
 V-0
@Thickness 0.750 mm
V-0
@Thickness 0.0295 in
ALL; UL 94
 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
ALL; UL 94
 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
ALL; UL 94
Glow Wire Ignition Temperature  725 °C
@Thickness 0.800 mm
1340 °F
@Thickness 0.0315 in
IEC 60695-2-13
 725 °C
@Thickness 1.60 mm
1340 °F
@Thickness 0.0630 in
IEC 60695-2-13
 750 °C
@Thickness 3.00 mm
1380 °F
@Thickness 0.118 in
IEC 60695-2-13
Glow Wire Flammability Index  960 °C
@Thickness 0.400 mm
1760 °F
@Thickness 0.0157 in
IEC 60695-2-12
 960 °C
@Thickness 0.800 mm
1760 °F
@Thickness 0.0315 in
IEC 60695-2-12
 960 °C
@Thickness 1.60 mm
1760 °F
@Thickness 0.0630 in
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
1760 °F
@Thickness 0.118 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 - 280 °C500 - 536 °F
Mold Temperature 60.0 - 90.0 °C140 - 194 °F
Drying Temperature 80.0 °C176 °F
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hour
Hold Pressure 40.0 - 90.0 MPa5800 - 13100 psi
 
Descriptive Properties
Comparative Tracking Index (CTI)PLC 1UL 746
FeaturesFlame Retardant
 Halogen Free
 Heat Stabilized
 Hydrolysis Resistant
FormsPellets
Generic MaterialNylon 66
Generic NamePolyamide 66 (Nylon 66)
Outdoor Suitabilityf1UL 746C; Black
Processing MethodExtrusion
 Injection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
RoHS ComplianceRoHS Compliant
UL File NumberE76261

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Bergamid™ A700 G25 HW UF Polyamide 66 (Nylon 66)
Avient Bergamid™ A70 G30 U Polyamide 66 (Nylon 66)
Avient Bergamid™ A700 G20 UF Polyamide 66 (Nylon 66)
Avient Bergamid™ A700 G20 U-SO Polyamide 66 (Nylon 66)
Avient Bergamid™ A70 G35 UF SO Polyamide 66 (Nylon 66)

PH0POL0775 / 145344

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.