MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient Bergamid™ A70 G35 UF SO Polyamide 66 (Nylon 66)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes:

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.47 g/cc
@Temperature 23.0 °C
0.0531 lb/in³
@Temperature 73.4 °F
±0.03 g/cm³; DIN 53479
Filler Content 35 %35 %Glass Fiber Reinforcement
Ash >= 35 %>= 35 %ISO 3451
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 130 MPa
@Thickness 4.00 mm,
Temperature 23.0 °C
18900 psi
@Thickness 0.157 in,
Temperature 73.4 °F
ISO 527-2/5
Elongation at Break 2.0 %
@Thickness 4.00 mm,
Temperature 23.0 °C
2.0 %
@Thickness 0.157 in,
Temperature 73.4 °F
ISO 527-2/5
Tensile Modulus 12.0 GPa
@Thickness 4.00 mm,
Temperature 23.0 °C
1740 ksi
@Thickness 0.157 in,
Temperature 73.4 °F
ISO 527-2/1
Charpy Impact Unnotched 5.00 J/cm²
@Temperature 23.0 °C
23.8 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 0.750 J/cm²
@Temperature 23.0 °C
3.57 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 60093
Comparative Tracking Index 600 V600 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 261 °C502 °FISO 3146
Maximum Service Temperature, Air 110 °C230 °FContinuous (GTP 50% Tensile); IEC 60216
 220 °C428 °FShort Time; IEC 60216
Deflection Temperature at 1.8 MPa (264 psi) 236 °C457 °FUnannealed; ISO 75-2/A
Flammability, UL94  V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
ALL; UL 94
 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
UL 94
Glow Wire Ignition Temperature 960 °C
@Thickness 0.800 - 3.00 mm
1760 °F
@Thickness 0.0315 - 0.118 in
0.8 mm wire; Ignition Temperature; IEC 60695-2-13
 
Descriptive Properties
FeaturesFlame Retardant
 Halogen Free
 Low (to None) Phosphorus Content
FormsPellets
Generic MaterialNylon 66
Generic NamePolyamide 66 (Nylon 66)
Regional AvailabilityEurope
RoHS ComplianceRoHS Compliant

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Bergamid™ A70 G35 H U BK SO Polyamide 66 (Nylon 66)
Avient Bergamid™ B70 G30 BK Polyamide 6 (Nylon 6), DAM
Avient OnFlex™ S KE 60A-3S1725 Thermoplastic Elastomer (TPE)
Avient Bergamid™ A70 G30 U Polyamide 66 (Nylon 66)
Avient Bergamid™ A700 G25 HW UF Polyamide 66 (Nylon 66)

PH0POL1397 / 145966

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.