MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient Bergamid™ A70 G35 H U BK SO Polyamide 66 (Nylon 66)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes:

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.50 g/cc0.0542 lb/in³ISO 1183
Filler Content 35 %35 %Glass Fiber Reinforcement
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm
@Thickness 4.00 mm,
Temperature 23.0 °C
0.0030 - 0.0050 in/in
@Thickness 0.157 in,
Temperature 73.4 °F
Flow Mold Shrinkage on Tensile Bar, flow Bergmann Method; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 130 MPa
@Thickness 4.00 mm,
Temperature 23.0 °C
18900 psi
@Thickness 0.157 in,
Temperature 73.4 °F
ISO 527-2
Elongation at Break 2.0 %
@Thickness 4.00 mm,
Temperature 23.0 °C
2.0 %
@Thickness 0.157 in,
Temperature 73.4 °F
ISO 527-2
Tensile Modulus 12.0 GPa
@Thickness 4.00 mm,
Temperature 23.0 °C
1740 ksi
@Thickness 0.157 in,
Temperature 73.4 °F
ISO 527-2
Charpy Impact Unnotched  4.00 J/cm²
@Temperature -30.0 °C
19.0 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 5.00 J/cm²
@Temperature 23.0 °C
23.8 ft-lb/in²
@Temperature 73.4 °F
Injection Molded; ISO 179
Charpy Impact, Notched  0.550 J/cm²
@Temperature -30.0 °C
2.62 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 0.750 J/cm²
@Temperature 23.0 °C
3.57 ft-lb/in²
@Temperature 73.4 °F
ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 60093
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 236 °C457 °FAnnealed; ISO 75-2/A
Flammability, UL94  V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
ALL; UL 94
 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
ALL; UL 94
 V-0
@Thickness 3.20 mm
V-0
@Thickness 0.126 in
ALL; UL 94
Glow Wire Flammability Index  960 °C
@Thickness 0.800 mm
1760 °F
@Thickness 0.0315 in
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
1760 °F
@Thickness 0.118 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 - 280 °C500 - 536 °F
Mold Temperature 65.0 - 85.0 °C149 - 185 °F
Drying Temperature 80.0 - 90.0 °C176 - 194 °F
Dry Time 4.00 hour4.00 hour
 
Descriptive Properties
AdditiveHeat Stabilizer
FeaturesFlame Retardant
FormsPellets
Generic MaterialNylon 66
Generic NamePolyamide 66 (Nylon 66)
Processing MethodInjection Molding
Regional AvailabilityEurope
RoHS ComplianceRoHS Compliant

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Bergamid™ A700 G25 HW UF Polyamide 66 (Nylon 66)
Avient Bergamid™ A70 G35 UF SO Polyamide 66 (Nylon 66)
Avient Bergamid™ A70 G30 U Polyamide 66 (Nylon 66)
Avient Bergamid™ A700 G20 U-SO Polyamide 66 (Nylon 66)
Avient Bergamid™ A700 G20 UF Polyamide 66 (Nylon 66)

PH0POL1325 / 145894

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.