MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Toyobo GLAMIDE® TY-592GHV 6T-Nylon
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon, Aromatic

Material Notes: GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing and a specific grade approved as UL94V-0 class is provided, and it exhibits excellent chemical resistance and oil resistance. Grade TY-592GHV is a flame resistant, aromatic 6T-Nylon. It is of halogen origin and contains 55% GF.

55

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.81 g/cc1.81 g/ccAbsolute Drying; ASTM-D792
Filler Content 55 %55 %
Water Absorption 0.10 %0.10 %Absolute Drying; ASTM-D570
Moisture Absorption at Equilibrium 0.80 %0.80 %Absolute Drying; ASTM-D570
Linear Mold Shrinkage  0.0010 - 0.0030 cm/cm
@Thickness 1.00 mm
0.0010 - 0.0030 in/in
@Thickness 0.0394 in
Absolute Drying
 0.0030 - 0.0060 cm/cm
@Thickness 3.00 mm
0.0030 - 0.0060 in/in
@Thickness 0.118 in
Absolute Drying
Melt Flow 4.0 g/10 min4.0 g/10 min
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 120120Absolute Drying; ASTM-D785
Tensile Strength, Ultimate  90.0 MPa
@Temperature 80.0 °C
13100 psi
@Temperature 176 °F
Practical Use (Water Absorption 0.8%); ASTM-D638
 170 MPa
@Temperature 80.0 °C
24700 psi
@Temperature 176 °F
Absolute Drying; ASTM-D638
 230 MPa
@Temperature 23.0 °C
33400 psi
@Temperature 73.4 °F
Practical Use (Water Absorption 0.8%); ASTM-D638
 245 MPa
@Temperature 23.0 °C
35500 psi
@Temperature 73.4 °F
Absolute Drying; ASTM-D638
 280 MPa
@Temperature -40.0 °C
40600 psi
@Temperature -40.0 °F
Practical Use (Water Absorption 0.8%); ASTM-D638
 295 MPa
@Temperature -40.0 °C
42800 psi
@Temperature -40.0 °F
Absolute Drying; ASTM-D638
Elongation at Break 1.8 %1.8 %Absolute Drying; ASTM-D638
Flexural Strength  125 MPa
@Temperature 80.0 °C
18100 psi
@Temperature 176 °F
Practical Use (Water Absorption 0.8%); ASTM-D790
 230 MPa
@Temperature 80.0 °C
33400 psi
@Temperature 176 °F
Absolute Drying; ASTM-D790
 310 MPa
@Temperature 23.0 °C
45000 psi
@Temperature 73.4 °F
Practical Use (Water Absorption 0.8%); ASTM-D790
 330 MPa
@Temperature 23.0 °C
47900 psi
@Temperature 73.4 °F
Absolute Drying; ASTM-D790
 380 MPa
@Temperature -40.0 °C
55100 psi
@Temperature -40.0 °F
Practical Use (Water Absorption 0.8%); ASTM-D790
 400 MPa
@Temperature -40.0 °C
58000 psi
@Temperature -40.0 °F
Absolute Drying; ASTM-D790
Flexural Modulus  8.10 GPa
@Temperature 80.0 °C
1170 ksi
@Temperature 176 °F
Practical Use (Water Absorption 0.8%); ASTM-D790
 15.0 GPa
@Temperature 80.0 °C
2180 ksi
@Temperature 176 °F
Absolute Drying; ASTM-D790
 17.0 GPa
@Temperature 23.0 °C
2470 ksi
@Temperature 73.4 °F
Practical Use (Water Absorption 0.8%); ASTM-D790
 17.5 GPa
@Temperature 23.0 °C
2540 ksi
@Temperature 73.4 °F
Absolute Drying; ASTM-D790
 18.0 GPa
@Temperature -40.0 °C
2610 ksi
@Temperature -40.0 °F
Practical Use (Water Absorption 0.8%); ASTM-D790
 19.0 GPa
@Temperature -40.0 °C
2760 ksi
@Temperature -40.0 °F
Absolute Drying; ASTM-D790
Izod Impact, Notched  1.40 J/cm
@Temperature -40.0 °C
2.62 ft-lb/in
@Temperature -40.0 °F
Absolute Drying; ASTM-D256
 1.40 J/cm
@Temperature -40.0 °C
2.62 ft-lb/in
@Temperature -40.0 °F
Practical Use (Water Absorption 0.8%); ASTM-D256
 1.50 J/cm
@Temperature 23.0 °C
2.81 ft-lb/in
@Temperature 73.4 °F
Absolute Drying; ASTM-D256
 1.80 J/cm
@Temperature 23.0 °C
3.37 ft-lb/in
@Temperature 73.4 °F
Practical Use (Water Absorption 0.8%); ASTM-D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+12 ohm-cm1.00e+12 ohm-cmASTM-D257
Dielectric Constant 4.3
@Frequency 1000 Hz
4.3
@Frequency 1000 Hz
Absolute Drying; ASTM-D150
Dielectric Strength  25.0 kV/mm
@Thickness 2.00 mm
635 kV/in
@Thickness 0.0787 in
Practical Use (Water Absorption 0.8%); ASTM-D149
 26.0 kV/mm
@Thickness 2.00 mm
660 kV/in
@Thickness 0.0787 in
Absolute Drying; ASTM-D149
Dissipation Factor 0.010
@Frequency 1000 Hz
0.010
@Frequency 1000 Hz
Absolute Drying; ASTM-D150
Arc Resistance 25 sec25 secASTM-D495
Comparative Tracking Index 350 V350 VIEC Method
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.0 µm/m-°C8.89 µin/in-°FAbsolute Drying; ASTM-D696
Deflection Temperature at 0.46 MPa (66 psi) >= 270 °C>= 518 °FAbsolute Drying; ASTM-D648
Deflection Temperature at 1.8 MPa (264 psi) 264 °C507 °FAbsolute Drying; ASTM-D648
Flammability, UL94 V-0V-0
 
Processing PropertiesMetricEnglishComments
Melt Temperature 310 - 330 °C590 - 626 °F
Mold Temperature 150 °C302 °F
Injection Pressure 135 MPa19600 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Toyobo GLAMIDE® TY-791GT 6T-Nylon
Toyobo GLAMIDE® TY-502NZ 6T-Nylon
Chemours Tefzel® HT-2004
Arkema Cristamid® MS 1700 Semi-Aromatic Nylon (PASA) (Dry)
Overview of materials for Nylon 66, Unreinforced

PTOY946 / 107497

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.