MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Toyobo GLAMIDE® TY-502NZ 6T-Nylon
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon, Aromatic

Material Notes: GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing and a specific grade approved as UL94V-0 class is provided, and it exhibits excellent chemical resistance and oil resistance. Grade TY-502NZ is a non-reinforced, aromatic 6T-Nylon with a high melting point.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.18 g/cc1.18 g/ccAbsolute Drying; ASTM-D792
Water Absorption 0.70 %0.70 %Absolute Drying; ASTM-D570
Moisture Absorption at Equilibrium 1.9 %1.9 %Absolute Drying; ASTM-D570
Linear Mold Shrinkage  0.0020 - 0.0040 cm/cm
@Thickness 1.00 mm
0.0020 - 0.0040 in/in
@Thickness 0.0394 in
Absolute Drying
 0.0050 - 0.0080 cm/cm
@Thickness 3.00 mm
0.0050 - 0.0080 in/in
@Thickness 0.118 in
Absolute Drying
Melt Flow 7.0 g/10 min7.0 g/10 min
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 120120Absolute Drying; ASTM-D785
Tensile Strength, Ultimate  28.0 MPa
@Temperature 80.0 °C
4060 psi
@Temperature 176 °F
Practical Use (Water Absorption 1.9%); ASTM-D638
 50.0 MPa
@Temperature 80.0 °C
7250 psi
@Temperature 176 °F
Absolute Drying; ASTM-D638
 85.0 MPa
@Temperature 23.0 °C
12300 psi
@Temperature 73.4 °F
Practical Use (Water Absorption 1.9%); ASTM-D638
 90.0 MPa
@Temperature 23.0 °C
13100 psi
@Temperature 73.4 °F
Absolute Drying; ASTM-D638
 106 MPa
@Temperature -40.0 °C
15400 psi
@Temperature -40.0 °F
Practical Use (Water Absorption 1.9%); ASTM-D638
 110 MPa
@Temperature -40.0 °C
16000 psi
@Temperature -40.0 °F
Absolute Drying; ASTM-D638
Elongation at Break 20 %20 %ASTM-D638
Flexural Strength  45.0 MPa
@Temperature 80.0 °C
6530 psi
@Temperature 176 °F
Practical Use (Water Absorption 1.9%); ASTM-D790
 80.0 MPa
@Temperature 80.0 °C
11600 psi
@Temperature 176 °F
Absolute Drying; ASTM-D790
 130 MPa
@Temperature 23.0 °C
18900 psi
@Temperature 73.4 °F
Practical Use (Water Absorption 1.9%); ASTM-D790
 145 MPa
@Temperature 23.0 °C
21000 psi
@Temperature 73.4 °F
Absolute Drying; ASTM-D790
 155 MPa
@Temperature -40.0 °C
22500 psi
@Temperature -40.0 °F
Practical Use (Water Absorption 1.9%); ASTM-D790
 160 MPa
@Temperature -40.0 °C
23200 psi
@Temperature -40.0 °F
Absolute Drying; ASTM-D790
Flexural Modulus  1.00 GPa
@Temperature 80.0 °C
145 ksi
@Temperature 176 °F
Practical Use (Water Absorption 1.9%); ASTM-D790
 2.50 GPa
@Temperature 80.0 °C
363 ksi
@Temperature 176 °F
Absolute Drying; ASTM-D790
 3.40 GPa
@Temperature 23.0 °C
493 ksi
@Temperature 73.4 °F
Practical Use (Water Absorption 1.9%); ASTM-D790
 3.50 GPa
@Temperature 23.0 °C
508 ksi
@Temperature 73.4 °F
Absolute Drying; ASTM-D790
 4.20 GPa
@Temperature -40.0 °C
609 ksi
@Temperature -40.0 °F
Practical Use (Water Absorption 1.9%); ASTM-D790
 4.50 GPa
@Temperature -40.0 °C
653 ksi
@Temperature -40.0 °F
Absolute Drying; ASTM-D790
Compressive Strength 100 MPa14500 psiAbsolute Drying; ASTM-D695
Izod Impact, Notched  0.600 J/cm
@Temperature 23.0 °C
1.12 ft-lb/in
@Temperature 73.4 °F
Practical Use (Water Absorption 1.9%); ASTM-D256
 0.700 J/cm
@Temperature -40.0 °C
1.31 ft-lb/in
@Temperature -40.0 °F
Practical Use (Water Absorption 1.9%); ASTM-D256
 0.700 J/cm
@Temperature -40.0 °C
1.31 ft-lb/in
@Temperature -40.0 °F
Absolute Drying; ASTM-D256
 1.20 J/cm
@Temperature 23.0 °C
2.25 ft-lb/in
@Temperature 73.4 °F
Absolute Drying; ASTM-D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+12 ohm-cm1.00e+12 ohm-cmASTM-D257
Dielectric Constant 4.0
@Frequency 1000 Hz
4.0
@Frequency 1000 Hz
ASTM-D150
Dielectric Strength  22.0 kV/mm
@Thickness 2.00 mm
559 kV/in
@Thickness 0.0787 in
Practical Use (Water Absorption 1.9%); ASTM-D149
 23.0 kV/mm
@Thickness 2.00 mm
584 kV/in
@Thickness 0.0787 in
Absolute Drying; ASTM-D149
Arc Resistance 130 sec130 secASTM-D495
Comparative Tracking Index >= 600 V>= 600 VIEC Method
 
Thermal PropertiesMetricEnglishComments
CTE, linear 55.0 µm/m-°C30.6 µin/in-°FAbsolute Drying; ASTM-D696
Deflection Temperature at 0.46 MPa (66 psi) 170 °C338 °FAbsolute Drying; ASTM-D648
Deflection Temperature at 1.8 MPa (264 psi) 100 °C212 °FAbsolute Drying; ASTM-D648
Flammability, UL94 HBHB
 
Processing PropertiesMetricEnglishComments
Melt Temperature 305 - 320 °C581 - 608 °F
Mold Temperature 90.0 °C194 °F
Injection Pressure 30.0 - 40.0 MPa4350 - 5800 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 6, Unreinforced
Toyobo GLAMIDE® TY-791GT 6T-Nylon
Toyobo GLAMIDE® TY-592GHV 6T-Nylon
Arkema Cristamid® MS 1700 Semi-Aromatic Nylon (PASA) (Dry)
Arkema Cristamid® MS 1100 Semi-Aromatic Nylon (PASA) (Dry)

PTOY916 / 107467

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.