MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Toyobo GLAMIDE® TY-502NZ 6T-Nylon
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon, Aromatic

Material Notes: GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing and a specific grade approved as UL94V-0 class is provided, and it exhibits excellent chemical resistance and oil resistance. Grade TY-502NZ is a non-reinforced, aromatic 6T-Nylon with a high melting point.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.18 g/ccAbsolute Drying; ASTM-D792
Water Absorption 0.70 %Absolute Drying; ASTM-D570
Moisture Absorption at Equilibrium 1.9 %Absolute Drying; ASTM-D570
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm
@Thickness 1.00 mm
Absolute Drying
 0.0050 - 0.0080 cm/cm
@Thickness 3.00 mm
Absolute Drying
Melt Flow 7.0 g/10 min
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 120Absolute Drying; ASTM-D785
Tensile Strength, Ultimate 28.0 MPa
@Temperature 80.0 °C
Practical Use (Water Absorption 1.9%); ASTM-D638
 50.0 MPa
@Temperature 80.0 °C
Absolute Drying; ASTM-D638
 85.0 MPa
@Temperature 23.0 °C
Practical Use (Water Absorption 1.9%); ASTM-D638
 90.0 MPa
@Temperature 23.0 °C
Absolute Drying; ASTM-D638
 106 MPa
@Temperature -40.0 °C
Practical Use (Water Absorption 1.9%); ASTM-D638
 110 MPa
@Temperature -40.0 °C
Absolute Drying; ASTM-D638
Elongation at Break 20 %ASTM-D638
Flexural Strength 45.0 MPa
@Temperature 80.0 °C
Practical Use (Water Absorption 1.9%); ASTM-D790
 80.0 MPa
@Temperature 80.0 °C
Absolute Drying; ASTM-D790
 130 MPa
@Temperature 23.0 °C
Practical Use (Water Absorption 1.9%); ASTM-D790
 145 MPa
@Temperature 23.0 °C
Absolute Drying; ASTM-D790
 155 MPa
@Temperature -40.0 °C
Practical Use (Water Absorption 1.9%); ASTM-D790
 160 MPa
@Temperature -40.0 °C
Absolute Drying; ASTM-D790
Flexural Modulus 1.00 GPa
@Temperature 80.0 °C
Practical Use (Water Absorption 1.9%); ASTM-D790
 2.50 GPa
@Temperature 80.0 °C
Absolute Drying; ASTM-D790
 3.40 GPa
@Temperature 23.0 °C
Practical Use (Water Absorption 1.9%); ASTM-D790
 3.50 GPa
@Temperature 23.0 °C
Absolute Drying; ASTM-D790
 4.20 GPa
@Temperature -40.0 °C
Practical Use (Water Absorption 1.9%); ASTM-D790
 4.50 GPa
@Temperature -40.0 °C
Absolute Drying; ASTM-D790
Compressive Strength 100 MPaAbsolute Drying; ASTM-D695
Izod Impact, Notched 60.0 J/m
@Temperature 23.0 °C
Practical Use (Water Absorption 1.9%); ASTM-D256
 70.0 J/m
@Temperature -40.0 °C
Practical Use (Water Absorption 1.9%); ASTM-D256
 70.0 J/m
@Temperature -40.0 °C
Absolute Drying; ASTM-D256
 120 J/m
@Temperature 23.0 °C
Absolute Drying; ASTM-D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+12 ohm-cmASTM-D257
Dielectric Constant 4.0
@Frequency 1000 Hz
ASTM-D150
Dielectric Strength 22.0 kV/mm
@Thickness 2.00 mm
Practical Use (Water Absorption 1.9%); ASTM-D149
 23.0 kV/mm
@Thickness 2.00 mm
Absolute Drying; ASTM-D149
Arc Resistance 130 secASTM-D495
Comparative Tracking Index >= 600 VIEC Method
 
Thermal PropertiesOriginal ValueComments
CTE, linear 55.0 µm/m-°CAbsolute Drying; ASTM-D696
Deflection Temperature at 0.46 MPa (66 psi) 170 °CAbsolute Drying; ASTM-D648
Deflection Temperature at 1.8 MPa (264 psi) 100 °CAbsolute Drying; ASTM-D648
Flammability, UL94 HB
 
Processing PropertiesOriginal ValueComments
Melt Temperature 305 - 320 °C
Mold Temperature 90.0 °C
Injection Pressure 30.0 - 40.0 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Nylon 6, Unreinforced
Toyobo GLAMIDE® TY-791GT 6T-Nylon
Toyobo GLAMIDE® TY-592GHV 6T-Nylon
Arkema Cristamid® MS 1700 Semi-Aromatic Nylon (PASA) (Dry)
Arkema Cristamid® MS 1100 Semi-Aromatic Nylon (PASA) (Dry)

PTOY916 / 107467

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.