MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Domo TechnylStar™ AFX 218 V50 PA6, 50% glass filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 50% Glass Fiber Filled

Material Notes: TECHNYLSTAR™ AFX 218 V50 is based on a patented high flow polyamide 66 resin, heat stabilized, reinforced with 50% of glass fiber, for injection molding. It is available in black and natural colors.

Benefits: Due to its outstanding flow characteristics, the product shows exceptional processing behavior and excellent surface aspect of the finished part.

Available in: Europe, Latin America and North America

Regulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applications.

Applications: The product is particularly suitable for all applications where a high rigidity is required: typically structural parts or brackets for the automotive industry. Its high mechanical performance allows that product to be an alternative to metal parts.

Product data for dry samples.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.57 g/cc0.0567 lb/in³ISO 1183/A
Water Absorption 0.60 %
@Temperature 23.0 °C,
Time 86400 sec
0.60 %
@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Linear Mold Shrinkage, Flow 0.0034 cm/cm0.0034 in/in
Linear Mold Shrinkage, Transverse 0.0042 cm/cm0.0042 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 255 MPa37000 psiISO 527 Type 1A
Tensile Stress at Strain  100 MPa
@Strain 1 %
14500 psi
@Strain 1 %
 145 MPa
@Strain 2 %
21000 psi
@Strain 2 %
 180 MPa
@Strain 3 %
26100 psi
@Strain 3 %
Elongation at Break 2.5 %2.5 %ISO 527 Type 1A
Tensile Modulus 17.0 GPa2470 ksiISO 527 Type 1A
Flexural Strength 380 MPa55100 psiISO 178
Flexural Modulus 15.0 GPa2180 ksiISO 178
Izod Impact, Notched (ISO) 17.0 kJ/m²8.09 ft-lb/in²ISO 180/1eA
Izod Impact, Unnotched (ISO) 88.0 kJ/m²41.9 ft-lb/in²ISO 180/1eU
Charpy Impact Unnotched 10.0 J/cm²47.6 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 1.50 J/cm²7.14 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 264 °C507 °FISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 256 °C493 °FISO 75/Af
Flammability, UL94 HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
1210
Glow Wire Ignition Temperature 675 °C
@Thickness 0.800 mm
1250 °F
@Thickness 0.0315 in
ISO 60695-2-12
Glow Wire Flammability Index 650 °C
@Thickness 0.800 mm
1200 °F
@Thickness 0.0315 in
ISO 60695-2-12
 
Processing PropertiesMetricEnglishComments
Feed Temperature 260 - 270 °C500 - 518 °F
Mold Temperature 60.0 - 90.0 °C140 - 194 °F
Drying Temperature 80.0 °C176 °F
Moisture Content <= 0.20 %<= 0.20 %
 
Descriptive Properties
Compression Zone270-280°C
Mixing Zone280-290°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® B3EG6 BK00564 30% Glass Filled PA6 (Dry)
Celanese VECTRA E115i LCP, 15% Glass Reinforced
BASF Ultramid® KR 4365 G5 BK 00100 35% Glass Filled PA6/6T FR (Dry)
Domo Technyl® C 218 V50 50% Glass Filled, Heat Stabilized Nylon 6
Domo TechnylStar™ SX 218 V50 PA6, 50% glass filled

PRHOD819 / 138050

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.