MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Devcon Underwater Repair Putty (UW) Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Emergency Repair Products

Comments: High-performance technology for repairing, patching and rebuilding equipment in habitually wet environments, even under water. Eliminates the need for substrate to be thoroughly dry before repairs. Invaluable for use in pulp and paper mills, wastewater treatment plants, and marine environments. Penetrates wetness to bond securely to steel, iron, aluminum, brass, bronze, concrete, wood, and some plastics. Non-rusting; easy to mix and apply. Cures in temperatures down to 40°F.

Data provided by Ellsworth Adhesives.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.63 g/cc0.0588 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8282ASTM D2240
Tensile Strength, Ultimate 19.0 MPa2760 psiASTM D638
Tensile Modulus 5.17 GPa750 ksiASTM D638
Flexural Yield Strength 34.4 MPa4990 psiASTM D790
Compressive Yield Strength 38.78 MPa5625 psiASTM D695
Adhesive Bond Strength 18.51 MPa2685 psiAdhesive tensile shear strength; ASTM D1002
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 8.68.6ASTM D150
Dielectric Strength 5.91 kV/mm150 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 32.0 µm/m-°C
@Temperature 20.0 °C
17.8 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Thermal Conductivity 0.590 W/m-K4.09 BTU-in/hr-ft²-°FASTM C177
Maximum Service Temperature, Air 93.3 °C200 °FOperating Temperature
Shrinkage 0.20 %0.20 %During Cure; ASTM D2566
 
Processing PropertiesMetricEnglishComments
Processing Temperature >= 4.44 °C>= 40.0 °F
Pot Life 45.0 min
@Temperature 23.9 °C
45.0 min
@Temperature 75.0 °F
 
Descriptive Properties
Coverage per lb.68 in²at 1/4 inch thick
Mix Ratio by Volume1 to 1resin:hardener
Mix Ratio by Weight1.4 to 1resin:hardener

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Epoxy Technology EPO-TEK® H61 Thermally Conductive Epoxy
Lehvoss LUVOCOM® 1105/CF/10/GR/10/TF/10-2 PEEK with carbon fiber, PTFE, lubricant modified
Evonik Vestoran® 1300-GF10 nf PPE
Evonik Vestoran® 1300-GF20 nf PPE
Lehvoss LUVOCOM® 1105/GF/20/EM PEEK with glass fiber

PITWX15 / 48502

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.