MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polimeros Mexicanos Rotolene® Black Plus Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Polyethylene compound specially formulated for rotational molding applications requiring good mechanical properties and good mold release properties. Rotational molded parts have smooth surface and texture finish when produced under optimal process conditions.

Formulated for manufacturing water tanks (less than 1200 liters capacity)offering good mechanical properties and durability.

Meets CONEG regulation for articles intended for direct food contact.

Information provided by Polimeros Mexicanos

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.330 - 0.390 g/cc0.0119 - 0.0141 lb/in³ASTM D1895
Density 0.937 g/cc0.0339 lb/in³ASTM D792
Particle Mesh Size 35 Mesh35 Meshless than 2%; ASTM D1921
Melt Flow 4.0 - 5.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
4.0 - 5.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Impact Test 61.0 J
@Temperature -40.0 °C
45.0 ft-lb
@Temperature -40.0 °F
0.125 in.; ARM test
 
Descriptive Properties
Pourability2.5 - 4 gr/s
ProcessRotational Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polimeros Mexicanos Rotolene® Industrial Black Linear Medium Density Polyethylene
Polimeros Mexicanos Rotolene® 93835-TG Medium Density Polyethylene
Polimeros Mexicanos Rotolene® 93050 Medium Density Polyethylene
Polimeros Mexicanos Rotolene® ECO-BLACK Linear Medium Density Polyethylene
Polimeros Mexicanos Rotolene® Natural Linear Medium Density Polyethylene

PMEXIC995 / 159906

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.