MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polimeros Mexicanos Rotolene® 93050 Medium Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Medium Density (MDPE); Linear Medium Density Polyethylene (LMDPE), Rotational Molded

Material Notes: Hexene Copolymer Linear Medium Density Polyethylene for rotational molding. This resin is fully UV8 stabilized.

Recommended for general purpose applications. Frequently used for water tanks (less than 2000 liters) and small to medium size containers exhibiting very good mechanical properties. When used for inner layers, it provides excellent smooth finish and texture.

Natural Polyethylene meets all requirements of US FDA as specified in 21 CFR 177.1520, covering safe use of polyolefin articles intended for direct food contact.

Information provided by Polimeros Mexicanos

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.330 - 0.390 g/cc0.0119 - 0.0141 lb/in³ASTM D1895
Density 0.935 g/cc0.0338 lb/in³ASTM D792
Particle Mesh Size 35 Mesh35 Meshless than 2%; ASTM D1921
ESCR 100% Igepal® >= 1000 hour>= 1000 hourASTM D1693
ESCR 10% Igepal® 300 hour300 hour
Melt Flow 5.2 g/10 min
@Load 2.16 kg,
Temperature 190 °C
5.2 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 18.6 MPa2700 psi50 mm/min; ASTM D638
Elongation at Yield 11.8 %11.8 %(2 in/min); ASTM D638
Flexural Modulus 0.689 GPa100 ksi1.3 mm/min; ASTM D790B
Impact Test 61.0 J
@Temperature -40.0 °C
45.0 ft-lb
@Temperature -40.0 °F
0.125 in.; ARM test
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 50.0 °C122 °FASTM D648
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
Pourability2.5 - 4 gr/s
ProcessRotational Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polimeros Mexicanos Rotolene® Natural Linear Medium Density Polyethylene
Polimeros Mexicanos Rotolene® 93835-TG Medium Density Polyethylene
Polimeros Mexicanos Rotolene® Industrial Black Linear Medium Density Polyethylene
Polimeros Mexicanos Rotolene® Black Plus Polyethylene
Polimeros Mexicanos Rotolene® ECO-BLACK Linear Medium Density Polyethylene

PMEXIC994 / 159905

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.