MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

Aremco Aremco-Bond™ 2320 High Performance Epoxide
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Toughened, Unfilled, Fast-Setting, BPA Free, 2:1, High Peel & Shear Strength

Vendors: Aremco’s High Performance Epoxies provide a wide range of solutions for bonding ceramics, composites, glass, metals, plastics, and other materials. Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/cc
Viscosity 35000 cP35000 cP
Linear Mold Shrinkage 0.0010 cm/cm0.0010 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7878
Shear Strength 33.09 MPa4800 psiASTM D1002-94
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+14 ohm-cm2.00e+14 ohm-cm
Dielectric Strength 43.3 kV/mm1100 kV/in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 59.4 µm/m-°C33.0 µin/in-°F
Maximum Service Temperature, Air 121 °C250 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  120 min
@Temperature 93.3 °C
2.00 hour
@Temperature 200 °F
alternate cure
 1440 - 2880 min
@Temperature 79.4 °C
24.0 - 48.0 hour
@Temperature 175 °F
recommended cure
Pot Life 60.0 min
@Temperature 25.0 °C
60.0 min
@Temperature 77.0 °F
100 gm mass
 
Descriptive Properties
Chemical ResistanceGood
ColorOff-White
Mix Ratio2:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aremco Aremco-Bond™ 2330 High Performance Epoxide
Aremco Aremco-Bond™ 2318 High Performance Epoxide
Armstrong A-7 Epoxy Adhesive
Aremco Aremco-Bond™ 855 Epoxy Adhesive
Aremco Aremco-Bond™ 597 Conductive Epoxy Adhesive

PAREM98 / 138445

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.