MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

Aremco Aremco-Bond™ 2318 High Performance Epoxide
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: High Temperature, Low Viscosity, Room Temperature Cure

Vendors: Aremco’s High Performance Epoxies provide a wide range of solutions for bonding ceramics, composites, glass, metals, plastics, and other materials. Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.58 g/cc1.58 g/cc
Viscosity 16000 cP16000 cPmixed viscosity
Linear Mold Shrinkage 0.0030 cm/cm0.0030 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8989
Flexural Strength 97.2 MPa14100 psiASTM D790
Shear Strength 7.826 MPa1135 psiASTM D1002-94
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.00e+15 ohm-cm3.00e+15 ohm-cm
Dielectric Constant 4.8
@Frequency 1000 Hz
4.8
@Frequency 1000 Hz
Dielectric Strength 18.1 kV/mm460 kV/in
Dissipation Factor 0.0140.014
 
Thermal PropertiesMetricEnglishComments
CTE, linear 70.2 µm/m-°C39.0 µin/in-°F
Thermal Conductivity 0.634 W/m-K4.40 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 120 °C248 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  120 min
@Temperature 93.3 °C
2.00 hour
@Temperature 200 °F
recommended cure
 240 min
@Temperature 20.0 °C
4.00 hour
@Temperature 68.0 °F
recommended cure
 1440 - 2880 min
@Temperature 23.0 °C
24.0 - 48.0 hour
@Temperature 73.4 °F
Pot Life 42.0 min
@Temperature 25.0 °C
42.0 min
@Temperature 77.0 °F
100 gm mass
 
Descriptive Properties
Chemical ResistanceExcellent
ColorBlack
Mix Ratio100:12

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aremco Aremco-Bond™ 526N High Performance Epoxide
Epoxy Technology EPO-TEK® H61 Thermally Conductive Epoxy
Raschig Group EPOXIDUR® 3580 EP Epoxy
Aremco Aremco-Bond™ 2330 High Performance Epoxide
Aremco Aremco-Bond™ 2320 High Performance Epoxide

PAREM97 / 138444

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.