MetalTek MTEK 375 Aluminum Bronze
Categories:
Metal
;
Nonferrous Metal
;
Copper Alloy
;
Bronze
Material Notes:
Engineered alloy for excellent wear and anti-galling properties in forming, bending and drawing dies. Aluminum Bronze heat treated to higher mechanical properties where necessary.
Information provided by MetalTek
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Mechanical Properties
Metric
English
Comments
Hardness, Brinell
>= 341
>= 341
3000 kg
352
352
3000 kg, typical
Component Elements Properties
Metric
English
Comments
Aluminum, Al
14.5 %
14.5 %
Copper, Cu
80 %
80 %
Iron, Fe
5.5 %
5.5 %
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Ampco Metal AMPCO® 26 Aluminum Bronze, Forging
MetalTek MTEK 230-N Cast UNS C95800 Nickel Aluminum Bronze
MetalTek MTEK 325 Aluminum Bronze
MetalTek MTEK 275 Cast UNS C95900 Aluminum Bronze
Overview of materials for Bronze
NMETEK011 / 18261
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.