MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Isopropanol ((CH3)2CHOH; 2-Propanol)
Categories: Fluid; Solvent

Key Words: dimethylcarbinol; isopropyl alcohol
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.7855 g/cc
@Temperature 20.0 °C
0.02838 lb/in³
@Temperature 68.0 °F
Viscosity 2.313 cP
@Temperature 20.0 °C
2.313 cP
@Temperature 68.0 °F
Dynamic Viscosity
Molecular Weight 60.11 g/mol60.11 g/mol
Vapor Pressure  0.044182 bar
@Temperature 20.0 °C
33.139 torr
@Temperature 68.0 °F
 0.1000 bar
@Temperature 33.6 °C
75.00 torr
@Temperature 92.5 °F
Surface Tension 21.79 dynes/cm
@Temperature 20.0 °C
21.79 dynes/cm
@Temperature 68.0 °F
 
Chemical PropertiesMetricEnglishComments
Critical Pressure 47.640 bar35733 torr
Critical Temperature 235.18 °C455.32 °F
Critical Density 0.271 g/cc0.00979 lb/in³
Critical Molar Volume 222 cm³/mol13.5 in³/mol
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 18.6
@Temperature 20.0 °C
18.6
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 90.0 J/g38.7 BTU/lbEnthalpy of fusion at normal melting point
Heat of Vaporization 663 J/g285 BTU/lbEnthalpy of vaporization at normal boiling temperature
Specific Heat Capacity 2.995 J/g-°C0.7158 BTU/lb-°F
 1.527 J/g-°C
@Temperature 25.0 °C
0.3650 BTU/lb-°F
@Temperature 77.0 °F
Vapor
Thermal Conductivity 0.135 W/m-K
@Temperature 25.0 °C
0.937 BTU-in/hr-ft²-°F
@Temperature 77.0 °F
Melting Point -87.9 °C-126 °FAt atmospheric pressure (760 torr)
Boiling Point 82.4 °C
@Pressure 0.101 MPa
180 °F
@Pressure 14.7 psi
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.3776
@Temperature 20.0 °C,
Wavelength 589.3 nm
1.3776
@Temperature 68.0 °F,
Wavelength 589.3 nm
Na D line
 
Descriptive Properties
Antoine's Vapor Pressure A Parameter18.6929
Antoine's Vapor Pressure B Parameter3640.2
Antoine's Vapor Pressure C Parameter-53.54
Antoine's Vapor Pressure Formulaln πp = A - B/(T+C)P in mmHg and T in K
CAS registry number (CARN)67-63-0
Chemical FormulaC3H8O
Critical Compressibility (Zc)0.248
Dipole moment (p/C.m)5.671E-28
Henry's Law Constant (atm m3/mol)7.89E-06
Molar Heat Capacity (298K)91.803 J/mol-K
Molar Heat Capacity of Vapor a Parameter32.4051
Molar Heat Capacity of Vapor b Parameter0.1884
Molar Heat Capacity of Vapor c Parameter6.402E-05
Molar Heat Capacity of Vapor d Parameter-9.255E-08
Molar Heat Capacity of Vapor FormulaCp = a + bT + cT2 + dT3Cp in J/mol-K
UN Number1219

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dimethyl Formamide (HCON(CH3)2; N,N-dimethylformamide; DMF)
Ethanol (CH3CH2OH; Ethyl Alcohol)
Ethylene glycol, C2H6O2
2-Octanol, C8H18O
2-Butoxyethanol, C6H14O2

VORG027 / 74538

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.