MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

409 Stainless Steel
Categories: Metal; Ferrous Metal; Heat Resisting; Stainless Steel; T 400 Series Stainless Steel

Material Notes: Titanium content ranges from 6 times C content to 0.75%. One of least expensive of stainless steels.

Applications: mufflers, exterior parts, non-critical corrosive applications.

Key Words: UNS S40900, ASME SA268, ASTM A176, ASTM A268, ASTM A651, SAE J405 (51409), DIN 1.4512, JIS SUH 409, B.S. 409 S 17, ferritic, ISO 4954 X6CrNb12, ISO 683/13 1Ti
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 7.80 g/cc0.282 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 448 MPa65000 psi
 30.0 MPa
@Temperature 870 °C
4350 psi
@Temperature 1600 °F
 61.0 MPa
@Temperature 760 °C
8850 psi
@Temperature 1400 °F
 148 MPa
@Temperature 650 °C
21500 psi
@Temperature 1200 °F
 254 MPa
@Temperature 540 °C
36800 psi
@Temperature 1000 °F
 326 MPa
@Temperature 425 °C
47300 psi
@Temperature 797 °F
 334 MPa
@Temperature 315 °C
48400 psi
@Temperature 599 °F
 365 MPa
@Temperature 205 °C
52900 psi
@Temperature 401 °F
 406 MPa
@Temperature 93.0 °C
58900 psi
@Temperature 199 °F
Tensile Strength, Yield 238 MPa
@Strain 0.2 %
34500 psi
@Strain 0.2 %
 19.0 MPa
@Strain 0.2 %,
Temperature 870 °C
2760 psi
@Strain 0.2 %,
Temperature 1600 °F
 39.0 MPa
@Strain 0.2 %,
Temperature 760 °C
5660 psi
@Strain 0.2 %,
Temperature 1400 °F
 92.0 MPa
@Strain 0.2 %,
Temperature 650 °C
13300 psi
@Strain 0.2 %,
Temperature 1200 °F
 136 MPa
@Strain 0.2 %,
Temperature 540 °C
19700 psi
@Strain 0.2 %,
Temperature 1000 °F
 165 MPa
@Strain 0.2 %,
Temperature 425 °C
23900 psi
@Strain 0.2 %,
Temperature 797 °F
 172 MPa
@Strain 0.2 %,
Temperature 205 °C
24900 psi
@Strain 0.2 %,
Temperature 401 °F
 172 MPa
@Strain 0.2 %,
Temperature 315 °C
24900 psi
@Strain 0.2 %,
Temperature 599 °F
 207 MPa
@Strain 0.2 %,
Temperature 93.0 °C
30000 psi
@Strain 0.2 %,
Temperature 199 °F
Elongation at Break 32.5 %32.5 %in 50 mm
 21 %
@Temperature 425 °C
21 %
@Temperature 797 °F
in 50 mm
 22.5 %
@Temperature 315 °C
22.5 %
@Temperature 599 °F
in 50 mm
 24 %
@Temperature 540 °C
24 %
@Temperature 1000 °F
in 50 mm
 25.5 %
@Temperature 205 °C
25.5 %
@Temperature 401 °F
in 50 mm
 29.5 %
@Temperature 93.0 °C
29.5 %
@Temperature 199 °F
in 50 mm
 44 %
@Temperature 650 °C
44 %
@Temperature 1200 °F
in 50 mm
 67.5 %
@Temperature 760 °C
67.5 %
@Temperature 1400 °F
in 50 mm
 75.5 %
@Temperature 870 °C
75.5 %
@Temperature 1600 °F
in 50 mm
Modulus of Elasticity 200 GPa29000 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000600 ohm-cm
@Temperature 20.0 °C
0.0000600 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.7 µm/m-°C
@Temperature 20.0 - 100 °C
6.50 µin/in-°F
@Temperature 68.0 - 212 °F
 11.9 µm/m-°C
@Temperature 20.0 - 260 °C
6.61 µin/in-°F
@Temperature 68.0 - 500 °F
 12.4 µm/m-°C
@Temperature 20.0 - 480 °C
6.89 µin/in-°F
@Temperature 68.0 - 896 °F
 12.9 µm/m-°C
@Temperature 20.0 - 650 °C
7.17 µin/in-°F
@Temperature 68.0 - 1200 °F
 13.5 µm/m-°C
@Temperature 20.0 - 815 °C
7.50 µin/in-°F
@Temperature 68.0 - 1500 °F
Specific Heat Capacity 0.460 J/g-°C
@Temperature 0.000 - 100 °C
0.110 BTU/lb-°F
@Temperature 32.0 - 212 °F
Thermal Conductivity  24.9 W/m-K
@Temperature 95.0 °C
173 BTU-in/hr-ft²-°F
@Temperature 203 °F
 28.6 W/m-K
@Temperature 540 °C
198 BTU-in/hr-ft²-°F
@Temperature 1000 °F
Melting Point 1425 - 1510 °C2597 - 2750 °F
Solidus 1425 °C2597 °F
Liquidus 1510 °C2750 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.080 %<= 0.080 %
Chromium, Cr 11.13 %11.13 %
Iron, Fe 86 %86 %
Manganese, Mn <= 1.0 %<= 1.0 %
Phosphorus, P <= 0.045 %<= 0.045 %
Silicon, Si <= 1.0 %<= 1.0 %
Sulfur, S <= 0.045 %<= 0.045 %
Titanium, Ti 0.75 %0.75 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
410 Stainless Steel
304 Stainless Steel
420 Stainless Steel
409 Stainless Steel, annealed sheet, strip, plate, bar
416 Stainless Steel

MQ409B / 12940

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.