MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Impet® 2700 GV1/45 (Europe) PET, 45% Glass Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), 50% Glass Reinforced

Material Notes: Polyethylene terephthalate, 45 % glass filled, high flowability, excellent gloss, high modulus, very high heat deflection temperature.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.74 g/cc0.0629 lb/in³ISO 1183
Moisture Absorption 0.150 %0.150 %23°C/50%RH; ISO 62
Viscosity Test 50 cm³/g0.50 dl/gISO 307, 1157, 1628
Linear Mold Shrinkage, Flow 0.0020 cm/cm0.0020 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0060 cm/cm0.0060 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 121121ISO 2039-2
Tensile Strength at Break 185 MPa26800 psi5mm/min; ISO 527-2/1A
Elongation at Break 1.5 %1.5 %5mm/min; ISO 527-2/1A
Tensile Modulus 17.0 GPa2470 ksi50mm/min; ISO 527-2/1A
Flexural Strength 240 MPa34800 psiISO 178
Flexural Modulus 17.0 GPa2470 ksiISO 178
Izod Impact, Notched (ISO) 13.0 kJ/m²6.19 ft-lb/in²ISO 180/1A
Charpy Impact Unnotched 3.50 J/cm²16.7 ft-lb/in²ISO 179/1eU
 3.10 J/cm²
@Temperature -30.0 °C
14.8 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 1.20 J/cm²5.71 ft-lb/in²ISO 179/1eA
 1.30 J/cm²
@Temperature -30.0 °C
6.19 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmIEC 60093
Surface Resistance >= 1.00e+14 ohm>= 1.00e+14 ohmIEC 60093
Dielectric Constant  4.5
@Frequency 1e+6 Hz
4.5
@Frequency 1e+6 Hz
IEC 60250
 5.2
@Frequency 100 Hz
5.2
@Frequency 100 Hz
IEC 60250
Dielectric Strength 35.0 kV/mm889 kV/inIEC 60243-1
Dissipation Factor  0.0030
@Frequency 100 Hz
0.0030
@Frequency 100 Hz
IEC 60250
 0.0165
@Frequency 1e+6 Hz
0.0165
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 175 V175 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 15.0 µm/m-°C8.33 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 100 µm/m-°C55.6 µin/in-°FISO 11359-2
Melting Point 248 °C478 °F10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 0.46 MPa (66 psi) 252 °C486 °FISO 75-1, -2
Deflection Temperature at 1.8 MPa (264 psi) 228 °C442 °FISO 75-1, -2
Deflection Temperature at 8.0 MPa 170 °C338 °FISO 75-1, -2
Vicat Softening Point 260 °C500 °FISO 306
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
Oxygen Index 26 %26 %ISO 4589
 
Processing PropertiesMetricEnglishComments
Processing Temperature 135 - 145 °C275 - 293 °Fcavity
 270 - 290 °C518 - 554 °Fhot runner
Feed Temperature 40.0 - 60.0 °C104 - 140 °F
Zone 1 260 - 270 °C500 - 518 °F
Zone 2 270 - 280 °C518 - 536 °F
Zone 3 280 - 290 °C536 - 554 °F
Zone 4 280 - 290 °C536 - 554 °F
Die Temperature 270 - 290 °C518 - 554 °F
Melt Temperature 270 - 290 °C518 - 554 °F
Drying Temperature 120 - 140 °C248 - 284 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Moisture Content <= 0.010 %<= 0.010 %
Screw Speed  50 rpm
@Diameter 55.0 mm
50 rpm
@Diameter 2.17 in
 65 rpm
@Diameter 40.0 mm
65 rpm
@Diameter 1.57 in
 80 rpm
@Diameter 25.0 mm
80 rpm
@Diameter 0.984 in
 
Descriptive Properties
Injection moldingYes
Injection speedfast

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Rynite® 545 NC010 PET-GF45
Celanese Impet® 2700 GV1/30 PET, 30% Glass Reinforced
Celanese Impet® 340R PET, 45% Glass Reinforced
EMS-Grivory Grivory® HT2V-3X V0 black 9021 PA6T/66-GF30
Akro-Plastic Akroloy® PA GF 50 (2706) PA 6.6 & PA6I/6T Conditioned, 50% Glass Filled

PHCQ442 / 178897

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.