MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Petromont 1100 High Density Polyethylene Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Petromont HDPE 1100 is a high-density polyethylene homopolymer resin produced using the UNIPOL® Process. This multi-purpose resin is intended primarily for use in most intermittent and continuous blow moulding equipment found in the industry.

Petromont HDPE 1100 has an intermediate molecular weight distribution. It combines maximum rigidity with high impact strength, top load strength, moderate swell, excellent colour and imparts no detectable taste or odour to packaged products.

Key Words: Dairy bottles
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.961 g/cc0.0347 lb/in³ASTM D1505
ESCR 100% Igepal® 15 hour15 hourF50; ASTM D1693-B
Melt Flow 0.70 g/10 min0.70 g/10 minI2; ASTM D1238
 50 g/10 min50 g/10 minI21; ASTM D238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6565ASTM D2240
Tensile Strength, Ultimate 20.7 MPa3000 psiASTM D638
Tensile Strength, Yield 30.1 MPa4370 psiASTM D638
Elongation at Break 750 %750 %ASTM D638
Flexural Modulus 1.725 GPa250.2 ksiASTM D790
Izod Impact, Notched 1.228 J/cm2.301 ft-lb/inASTM D256
 1.015 J/cm
@Temperature 0.000 °C
1.902 ft-lb/in
@Temperature 32.0 °F
ASTM D256
Elmendorf Tear Strength, MD 1.97 g/micron50.0 g/milASTM D1922
 
Thermal PropertiesMetricEnglishComments
CTE, linear 150 µm/m-°C
@Temperature 20.0 °C
83.3 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Melting Point 133 °C271 °FPetromont
Crystallization Temperature 119 °C246 °FPetromont
Deflection Temperature at 0.46 MPa (66 psi) 99.0 °C210 °FASTM D648
Vicat Softening Point 130 °C266 °FASTM D1525
Brittleness Temperature <= -76.0 °C<= -105 °FASTM D746
 
Descriptive Properties
ProcessBlow Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Maxxam™ DP 9052-3-1000 Polyethylene, High Density (HDPE)
Equate EPDA-5040 HDPE Non-Pressure Gravity Pipe Resin
SCG Chemicals EL-Lene™ H6240B High Density Polyethylene Blow Molding
Overview of materials for High Density Polyethylene (HDPE), Extruded
Overview of materials for Polypropylene, Extrusion Grade

PPETROM03 / 56197

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.