MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Equate EPDA-5040 HDPE Non-Pressure Gravity Pipe Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: EPDA-5040 is a high molecular weight high density polyethylene copolymer resin designed for non-pressure gravity pipe applications. It has a good balance of flexibility, ductility, stiffness and toughness for exceptional freedom in pipe designing. It also offers excellent resistance to environmental stress cracking. EPDA-5040 has been adequately stabilized for long-term service life durability. The broad molecular weight distribution provides for easy processability in to pipe with smooth pipe surfaces and good dispersion of pigments, and carbon black for protection against UV.

Applications: EPDA-5040 applications include gravity pipe systems for underground drainage and sewage. It is suitable for both straight and structured wall pipes and for extruding electrical conduits

Information provided by Equate

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.952 g/cc0.0344 lb/in³ASTM D792
ESCR 100% Igepal® >= 1000 hour
@Temperature 50.0 °C
>= 1000 hour
@Temperature 122 °F
ASTM D1693 B
High Load Melt Index 10 g/10 min
@Load 21.0 kg
10 g/10 min
@Load 46.3 lb
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 35.0 MPa5080 psiASTM D638
Tensile Strength, Yield 26.0 MPa3770 psiASTM D638
Elongation at Break >= 750 %>= 750 %ASTM D638
Flexural Modulus 1.18 GPa171 ksiASTM D790
Izod Impact, Unnotched (ISO) 17.0 kJ/m²8.09 ft-lb/in²ASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear 150 µm/m-°C83.3 µin/in-°FASTM D969
Melting Point 135 °C275 °FEquate Test Method
Crystallization Temperature 113 °C235 °FEquate Test Method
Deflection Temperature at 0.46 MPa (66 psi) 99.0 °C210 °FASTM D648
Vicat Softening Point 130 °C266 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Zone 1 200 °C392 °F
Zone 2 205 °C401 °F
Zone 3 205 °C401 °F
Zone 4 205 °C401 °F
Adapter Temperature 205 °C401 °F
Die Temperature 205 °C401 °F
Melt Temperature 210 °C410 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Maxxam™ DP 9052-3-1000 Polyethylene, High Density (HDPE)
Petromont 1100 High Density Polyethylene Resin
Chevron Phillips Marlex® HP076 High Density Polyethylene, Pipe Grade
Petromont 4100 High Density Polyethylene Resin
Equate EMDA-6147 HDPE Blow Molding Resin

PEQUAT905 / 150433

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.