MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow DOWLEX™ 2071 Linear Low Density Polyethylene
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: DOWLEX® 2071 Polyethylene resin is a linear low density polyethylene resin specifically designed for the manufacture of high strength, thin gauge films for use in applications such as grocery sacks and trash bags. It contains high level of slip additive and medium level of antiblock additive. It complies with U.S. FDA regulation 21 CFR 177.1520 c 3.1 (a) for food packaging applications. The regulation should be consulted for complete details.

Film properties below based on a film thickness of 38 µm. Data provided by Dow Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.928 g/cc0.0335 lb/in³
Thickness 38.0 microns1.50 mil
Melt Flow 0.85 g/10 min
@Load 2.16 kg
0.85 g/10 min
@Load 4.76 lb
Melt flow ratio I10/I2 is 8.5.
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 13.0 MPa1890 psi
Film Tensile Strength at Yield, TD 15.0 MPa2180 psi
Coefficient of Friction 0.200.20
Elmendorf Tear Strength MD 350 g350 g
Elmendorf Tear Strength TD 940 g940 g
Elmendorf Tear Strength, MD 9.20 g/micron234 g/mil
Elmendorf Tear Strength, TD 24.7 g/micron627 g/mil
Dart Drop 5.90 g/micron150 g/mil
Film Tensile Strength at Break, MD 40.0 MPa5800 psi
Film Tensile Strength at Break, TD 31.0 MPa4500 psi
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 112 °C234 °F
 
Optical PropertiesMetricEnglishComments
Haze 10 %10 %
Gloss 28 %28 %45°
 
Processing PropertiesMetricEnglishComments
Processing Temperature 226 °C439 °FFilm extrusion temperature
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow DOWLEX™ 2045G Linear Low Density Polyethylene
Dow DOWLEX™ 2045A Linear Low Density Polyethylene, Blown Film Grade
Dow DOWLEX™ 2056 Linear Low Density Polyethylene, Heavy Duty Film Grade
Dow DOWLEX™ 2070D Linear Low Density Polyethylene, Blown Film Grade
Dow DOWLEX™ 2027A Linear Low Density Polyethylene, Cast Film Grade

PDW440 / 34509

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.