MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

RSP Technology RSA-8009 AE Aluminum Super Alloy
Categories: Metal; Nonferrous Metal; Aluminum Alloy

Material Notes: High strength and fatigue at elevated temperatures, typically 200 - 400C

Applications:

  • Impellors, pump housings, valves, vanes, pistons
  • Missile vins, rims
Replacing: Titanium, Stainless steel, Conventional al alloys like 2618, 2014, 4032

RSP Technology develops, produces and sells aluminium super alloys with high end properties. By using its own Meltspinning process, ultra fast cooling rates can be reached, converting more than 1 million degrees per second. As a result very fine nanostructured alloys with new functionalities are being developed and produced.

Information provided by RSP Technology BV

Key Words: AA8009
Vendors: RSP Technology – Aluminum as strong as Titanium For more information contact: +31 (0)596 632 300 or visit www.rsp-technology.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 2.94 g/cc0.106 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 140140
Tensile Strength, Ultimate 450 MPa65300 psi
 270 MPa
@Temperature 300 °C,
Time 3.60e+6 sec
39200 psi
@Temperature 572 °F,
Time 1000 hour
 310 MPa
@Temperature 250 °C,
Time 3.60e+6 sec
45000 psi
@Temperature 482 °F,
Time 1000 hour
 350 MPa
@Temperature 200 °C,
Time 3.60e+6 sec
50800 psi
@Temperature 392 °F,
Time 1000 hour
 380 MPa
@Temperature 150 °C,
Time 3.60e+6 sec
55100 psi
@Temperature 302 °F,
Time 1000 hour
 410 MPa
@Temperature 100 °C,
Time 3.60e+6 sec
59500 psi
@Temperature 212 °F,
Time 1000 hour
Tensile Strength, Yield 375 MPa54400 psi
 240 MPa
@Temperature 300 °C
34800 psi
@Temperature 572 °F
 275 MPa
@Temperature 250 °C
39900 psi
@Temperature 482 °F
 310 MPa
@Temperature 200 °C
45000 psi
@Temperature 392 °F
 350 MPa
@Temperature 150 °C
50800 psi
@Temperature 302 °F
 370 MPa
@Temperature 100 °C
53700 psi
@Temperature 212 °F
Elongation at Break 15 %15 %
Tensile Modulus 90.0 GPa13100 ksi
Fatigue Strength 160 MPa
@Temperature 250 °C
23200 psi
@Temperature 482 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 19.0 µm/m-°C10.6 µin/in-°F
Thermal Conductivity 115 W/m-K798 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 88.2 %88.2 %as balance
Iron, Fe 8.7 %8.7 %
Silicon, Si 1.8 %1.8 %
Vanadium, V 1.3 %1.3 %
 
Descriptive Properties
Specific Stiffness31GPa/(g/cc)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RSP Technology RSA-905 AE Aluminum Super Alloy
RSP Technology RSA-4019 AE Aluminum Super Alloy
RSP Technology RSA-443 AE Aluminum Super Alloy
RSP Technology RSA-6061 T6 Aluminum Super Alloy
Aluminum 7075-T6; 7075-T651

NRSP23 / 100837

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.