MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ThyssenKrupp SECURE 400 Structural Steel
Categories: Metal; Ferrous Metal; Carbon Steel; Low Carbon Steel

Material Notes: This Material Specification applies to the alloyed, liquid-quenched and tempered high-strength special steel SECURE 400 for civil use, this is usually produced in thickness from 3 mm up to 50 mm.

Application: The steels may be used for purposes of ballistic protection mainly for applications like armoured limousines and valuable transporters.

Information Provided by Thyssen Krupp

Key Words: 30CrMoNb5-2
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 1150 MPa167000 psi
Tensile Strength, Yield 950 MPa138000 psi
Elongation at Break 11 %11 %
Charpy Impact 20.0 J
@Temperature -40.0 °C
14.8 ft-lb
@Temperature -40.0 °F
Transverse
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 1.5 %<= 1.5 %
Carbon, C <= 0.32 %<= 0.32 %
Chromium, Cr <= 1.5 %<= 1.5 %
Iron, Fe >= 94.1 %>= 94.1 %As Balance
Manganese, Mn <= 1.0 %<= 1.0 %
Molybdenum, Mo <= 0.50 %<= 0.50 %
Nickel, Ni <= 0.70 %<= 0.70 %
Phosphorus, P <= 0.015 %<= 0.015 %
Silicon, Si <= 0.40 %<= 0.40 %
Sulfur, S <= 0.0050 %<= 0.0050 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ThyssenKrupp SECURE 500 Structural Steel
ThyssenKrupp XAR® 400 Structural Steel
Wingate Alloys Winco-Tuf 40IT Ultra High Strength, Thru-Hardened Alloy Wear Plate
AISI Type S1 Tool Steel, quenched 955°C (1750°F), tempered 150°C (300°F)
ASTM A36 Steel, bar

NTHYSS040 / 90360

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.