MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ThyssenKrupp XAR® 400 Structural Steel
Categories: Metal; Ferrous Metal; Carbon Steel; Low Carbon Steel

Material Notes: This Material Specification applies to 3 to 100 mm thick plates of the wear-resistant special structural steel XAR® 400.

Application: The steel may be used for wear exposed structures, e.g. excavating, mining and earth-moving machinery, truck dump bodies, conveying, crushing and pulverizing equipment, scrap presses, paving moulds and in switch manufacturing.

Information Provided by Thyssen Krupp

Key Words: EN 1.8714
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 1250 MPa181000 psi
Tensile Strength, Yield 1050 MPa152000 psi
Elongation at Break 12 %12 %
Charpy Impact 30.0 J
@Temperature -40.0 °C
22.1 ft-lb
@Temperature -40.0 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 1.0 %<= 1.0 %
Boron, B <= 0.0050 %<= 0.0050 %
Carbon, C <= 0.20 %<= 0.20 %
Chromium, Cr <= 1.0 %<= 1.0 %
Iron, Fe >= 94.5 %>= 94.5 %As Balance
Manganese, Mn <= 1.5 %<= 1.5 %
Molybdenum, Mo <= 0.50 %<= 0.50 %
Other <= 0.48 %<= 0.48 %Carbon Equivalent
Phosphorus, P <= 0.025 %<= 0.025 %
Silicon, Si <= 0.80 %<= 0.80 %
Sulfur, S <= 0.010 %<= 0.010 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ThyssenKrupp SECURE 400 Structural Steel
ThyssenKrupp COR-TEN A Structural Steel
ThyssenKrupp PAS 420 Structural Steel for Cold Forming
ThyssenKrupp XABO® 460 Structural Steel
304 Stainless Steel

NTHYSS025 / 90345

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.