MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 1200 T-70A UV Ether-based Thermoplastic Polyurethane Elastomer (; UV Stabilized
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Ether Grade

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.06 g/cc1.06 g/ccASTM D 792
Linear Mold Shrinkage 0.0050 - 0.015 cm/cm
@Thickness 3.20 mm
0.0050 - 0.015 in/in
@Thickness 0.126 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 70
@Time 10.0 sec
70
@Time 0.00278 hour
ASTM D 2240
Tensile Strength at Break 15.2 MPa
@Thickness 3.20 mm
2200 psi
@Thickness 0.126 in
Die C; 20 in/min (500 mm/min); ASTM D 412
Elongation at Break >= 500 %
@Thickness 3.20 mm
>= 500 %
@Thickness 0.126 in
Die C, 20 in/min (500 mm/min); ASTM D 412
Tear Strength 70.1 kN/m400 pliDie C; ASTM D 624
 
Processing PropertiesMetricEnglishComments
Melt Temperature 185 - 218 °C365 - 425 °F
Mold Temperature 37.8 - 60.0 °C100 - 140 °F
Drying Temperature 107 °C
@Time 21600 sec
225 °F
@Time 6.00 hour
Moisture Content 0.010 %0.010 %
Dew Point -17.8 °C0.000 °F
Injection Pressure 68.9 - 103 MPa10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Clariant Renol PURSP0002 Polyurethane Elastomer, Ether Based
RTP Company RTP 1200 T-70A Z NATURAL Ether-based Thermoplastic Polyurethane Elastomer (; Translucent
Huntsman IROGRAN® A 75 P 4665N TPU-Polyether
Huntsman IROGRAN® A 65 P 4324 N TPU-Polyether
Lubrizol ESTANE® 58309 Ether Based Thermoplastic Polyurethane

PQZUA20204 / 134741

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.