MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient Elastamax™ XL 0122-70 SEBS-Based Thermoplastic Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: This is a soft, clear thermoplastic elastomer based on SEBS technology. It is intended for injection molding. Physical Form: Pellet. Standard Color: Clear.

Information provided by M. A. Hanna. M. A. Hanna and Geon merged to form PolyOne in 2000.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.890 g/cc0.0322 lb/in³ASTM D792
Melt Flow  41 g/10 min
@Load 2.16 kg,
Temperature 190 °C
41 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 228 g/10 min
@Load 5.00 kg,
Temperature 190 °C
228 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 24245 sec. delay; ASTM D2240
Tensile Strength, Ultimate 7.20 MPa1040 psi10 in/min; ASTM D412
Elongation at Break 1213 %1213 %10 in/min; ASTM D412
50% Modulus 0.340 MPa
@Strain 50 %
0.340 MPa
@Strain 50 %
10 in/min; ASTM D412
100% Modulus 0.510 MPa
@Strain 100 %
74.0 psi
@Strain 100 %
ISO 37
200% Modulus 0.810 MPa
@Strain 200 %
117 psi
@Strain 200 %
10 in/min; ASTM D412
300% Modulus 1.17 MPa
@Strain 300 %
170 psi
@Strain 300 %
10 in/min; ASTM D412
Tear Strength 20.7 kN/m118 pliDie 'C' Tear; 20 in/min; ASTM D624

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teknor Apex TEKRON® 4000-25 Thermoplastic Elastomer
ExxonMobil Santoprene® 281-64MED Thermoplastic Elastomer
Dynasol Solprene® 4318 Thermoplastic Rubber SBS Dry
Clariant Renol PURSP0002 Polyurethane Elastomer, Ether Based
Avient Elastamax™ XL 0135-37 SEBS-Based Thermoplastic Elastomer

PHG156 / 46824

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.