MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Abatron AboCast 8-2/Abocure 8-2 Epoxy  (discontinued **)
Categories: Polymer; Thermoset; Epoxy

Material Notes: 2-part solvent-free dielectric epoxy casting compound.

Processing: 100/50 ratio (pbw); Gel time, 100 g (3.5 oz.): 265 minutes; cures in 3 weeks at 25°C (77°F).

Applications: solventless casting, adhesive, and coating.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Absorption 0.21 %0.21 %in 24 hours.
Viscosity Measurement 16001600
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8282
Tensile Strength, Ultimate 62.05 MPa9000 psi
Elongation at Break 4.0 %4.0 %
Flexural Strength 102.04 MPa14800 psi
Izod Impact, Notched 0.272 J/cm0.510 ft-lb/in
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity  5.00e+11 ohm-cm
@Temperature 93.3 °C
5.00e+11 ohm-cm
@Temperature 200 °F
 1.00e+13 ohm-cm
@Temperature 65.6 °C
1.00e+13 ohm-cm
@Temperature 150 °F
 3.00e+15 ohm-cm
@Temperature 25.0 °C
3.00e+15 ohm-cm
@Temperature 77.0 °F
Dielectric Constant 3.41
@Frequency 1e+6 Hz
3.41
@Frequency 1e+6 Hz
Dissipation Factor 0.012
@Frequency 1e+6 Hz
0.012
@Frequency 1e+6 Hz
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 62.0 °C144 °FDeflection temperature; load unknown.
 
Processing PropertiesMetricEnglishComments
Processing Temperature 25.0 °C77.0 °FCuring time: 3 weeks

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arlon Electronic Materials 45N Multifunctional Epoxy Laminate and Prepreg
Armstrong A-1/A Epoxy Adhesive
Atom Adhesives AA-BOND F110 Epoxy Adhesive
Cosmic Plastics CP7314 Epoxy Molding Compound
Overview of materials for Epoxy Adhesive

PABCH1 / 21962

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.