MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Master Bond EP21 Room Temperature Curing Two Component Epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: Key Features:
  • Moderate viscosity
  • Electrically insulative
  • Room temperature curing
  • One to one mix ratio — rigid to flexible cure
  • Shore D hardness >70
  • Dimensionally stable
Product Description: Master Bond EP21 is a two component, room temperature curing epoxy adhesive, sealant, coating, and encapsulating system featuring outstanding physical properties, superb dimensional stability and low shrinkage upon curing. This moderate viscosity system has a very forgiving 1 to 1 mix ratio by weight or volume. In fact, EP21 has the unusual feature of allowing the properties of the cured system to be altered by tweaking the mix ratio. Adding more Part A (maximum allowed 2:1 mix ratio by weight) will give a more rigid cure, which allows for better machinability. Adding more Part B (maximum 1:2 mix ratio by weight) offers a more forgiving cure, allowing for enhanced impact and shock resistance. It bonds well to a variety of substrates including metals, composites, glass, ceramics and many rubbers and plastics. EP21 features solid thermal cycling resistance. It also withstands many chemicals including water, oils, fuels and many acids and bases. It is serviceable over the wide temperature range of -60°F to +250°F. Once cured, EP21 is a highly reliable electrical insulator. EP21 is truly a versatile system and can be used in electronic, electrical, aerospace, optical and OEM applications, among others.

Product Advantages:

  • Convenient mixing: non-critical 1:1 mix ratio by weight or volume
  • Variable mix ratio feature allows adjusting the type of Cure
  • First rate physical strength properties
  • Moderate viscosity; even and smooth flow
  • Sound dimensional stability; low shrinkage upon Curing
  • Sterling electrical insulation properties

Information provided by Master Bond Inc.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Viscosity 28000 - 42000 cP28000 - 42000 cPPart A
 45000 - 65000 cP45000 - 65000 cPPart B
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 45 - 5045 - 50
Tensile Strength >= 55.2 MPa>= 8000 psi
Tensile Modulus >= 2.76 GPa>= 400 ksi
Adhesive Bond Strength >= 20.7 MPa>= 3000 psiTensile lap, Aluminum to Aluminum
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cm
Dielectric Constant 2.9
@Frequency 60 Hz
2.9
@Frequency 60 Hz
Dielectric Strength >= 17.3 kV/mm
@Thickness 3.17 mm
>= 440 kV/in
@Thickness 0.125 in
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °F
Minimum Service Temperature, Air -51.1 °C-60.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 120 - 180 min2.00 - 3.00 hourOptimum cure: overnight at RT, plus 150-200°F
 120 - 180 min
@Temperature 93.3 °C
2.00 - 3.00 hour
@Temperature 200 °F
 2880 - 4320 min
@Temperature 23.9 °C
48.0 - 72.0 hour
@Temperature 75.0 °F
Working Life 90.0 - 120 min90.0 - 120 minAfter mixing, 100 g batch
Shelf Life 12.0 Month
@Temperature <=23.9 °C
12.0 Month
@Temperature <=75.0 °F
in original, unopened containers
 
Descriptive Properties
Mixing Ratio1:1 by weight for volumeParts A to B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Master Bond EP21ND Non Drip Room Temperature Curing Epoxy System
DuPont Mobility and Materials Betamate™ XW 1185 Epoxy
Master Bond EP42HT-2AO-1 Two Part, Cryogenically Serviceable Epoxy
Master Bond EP42HT-2AO Two Component, Thermally Conductive, Heat Resistant Epoxy
Master Bond EP40 High Shear and Peel Strength, Two Component, Flexible Epoxy

PMASTM814 / 185407

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.