MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Toppyl PB 1600M Polybutene  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polybutene

Material Notes: Polybutene-1 (PB-1) grade Toppyl PB 1600M is a formulated random copolymer of butene-1 with low ethylene content and contains both slip and antilock. In blends with PE polymers, it forms a separate, but well-dispersed phase. Its primary use is as a minority blend component in the seal layer of easy-opening packaging films, produced by blow n film extrusion. A typical PE blend partner for Toppyl PB 1600M could be any ethylene homo-or copolymer in the melt index range of 0.5 to 2.0 g/10min. Applications: Bags & Pouches, Food Packaging Film, Lamination Film, Peelable Film, Secondary Packaging, Specialty Film

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.913 g/cc0.0330 lb/in³ISO 1183-1
Melt Flow  1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133-1
 30 g/10 min
@Load 10.0 kg,
Temperature 190 °C
30 g/10 min
@Load 22.0 lb,
Temperature 374 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 30.0 MPa4350 psiISO 8986-2
Elongation at Break 300 %300 %ISO 8986-2
Flexural Modulus 0.250 GPa36.3 ksiISO 178
 
Thermal PropertiesMetricEnglishComments
Melting Point 97.0 °C207 °FTm2; ISO 11357-3
 115 °C239 °FTm1; ISO 11357-3
 
Descriptive Properties
Processing MethodBlown Film

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil EXACT™ 4150 Plastomer
ExxonMobil Escorene® LD 713.93 Cast Film Resin
Lushan EV1050G1/RF EVA Film for Encapsulating Solar modules, Reinforced Friendly
LG Chemical SEETEC EF321 Ethylene Vinyl Acetate
ExxonMobil Optema® TC-114 Cast Ethylene Methyl Acrylate

PEQT8587 / 220222

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.