MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Bohler-Uddeholm BÖHLER M268 VMR® Plastic Mold Steel
Categories: Metal; Ferrous Metal; Tool Steel; Mold Steel

Material Notes: Description: HBÖHLER M268 VMR is a hardened and tempered plastic mould steel with excellent cleanliness for best polishability. The hardness is constant over the entire cross-section of the steel block, even at large sizes, due to the addition of nickel.

Applications: Moulds for plastics processing, components for general mechanical engineering and tool manufacture where highest polishability and fatigue strength are required.

Key Words: EN 1.2738; AISI P20; 40CrMnNiMo8-6-4
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.85 g/cc0.284 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 310 - 350310 - 350
Modulus of Elasticity 210 GPa30500 ksi
 
Thermal PropertiesMetricEnglishComments
CTE, linear  12.8 µm/m-°C
@Temperature 100 °C
7.11 µin/in-°F
@Temperature 212 °F
 13.0 µm/m-°C
@Temperature 200 °C
7.22 µin/in-°F
@Temperature 392 °F
 13.8 µm/m-°C
@Temperature 300 °C
7.67 µin/in-°F
@Temperature 572 °F
 14.0 µm/m-°C
@Temperature 400 °C
7.78 µin/in-°F
@Temperature 752 °F
 14.2 µm/m-°C
@Temperature 500 °C
7.89 µin/in-°F
@Temperature 932 °F
 14.2 µm/m-°C
@Temperature 600 °C
7.89 µin/in-°F
@Temperature 1110 °F
 14.5 µm/m-°C
@Temperature 700 °C
8.06 µin/in-°F
@Temperature 1290 °F
Specific Heat Capacity 0.460 J/g-°C0.110 BTU/lb-°F
Thermal Conductivity  28.0 W/m-K
@Temperature 700 °C
194 BTU-in/hr-ft²-°F
@Temperature 1290 °F
 31.1 W/m-K
@Temperature 600 °C
216 BTU-in/hr-ft²-°F
@Temperature 1110 °F
 32.8 W/m-K
@Temperature 500 °C
228 BTU-in/hr-ft²-°F
@Temperature 932 °F
 33.9 W/m-K
@Temperature 400 °C
235 BTU-in/hr-ft²-°F
@Temperature 752 °F
 34.3 W/m-K
@Temperature 20.0 °C
238 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
 34.8 W/m-K
@Temperature 300 °C
242 BTU-in/hr-ft²-°F
@Temperature 572 °F
 35.1 W/m-K
@Temperature 100 °C
244 BTU-in/hr-ft²-°F
@Temperature 212 °F
 35.3 W/m-K
@Temperature 200 °C
245 BTU-in/hr-ft²-°F
@Temperature 392 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.38 %0.38 %
Chromium, Cr 2.0 %2.0 %
Iron, Fe 94.52 %94.52 %As remainder
Manganese, Mn 1.5 %1.5 %
Molybdenum, Mo 0.20 %0.20 %
Nickel, Ni 1.1 %1.1 %
Silicon, Si 0.30 %0.30 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI Type P20 Mold Steel (UNS T51620)
Bohler-Uddeholm IMPAX® P20 Hot Work Tool Steel
Bohler-Uddeholm P20 PREMIUM MODIFIED Pre-hardened Mold Steel
Industeel CLC 1.2738 Prehardened Mold Steel (300HB/30HRC) for Thick Sections
EDRO #3 Prehardened Mold Quality P20 Alloy Steel

NBUCOR69 / 133742

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.