MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LATI LATISHIELD 87/28-06A Polycarbonate E.M.I. Shielding Plastic  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Material Notes: Description: Latishield E.M.I. shielding materials were developed to solve the problem of shielding electromagnetic interferences with plastic components. The answer is a mixture of two different types of granules, resulting in a homogeneous distribution of the shielding fiber reinforcement throughout the polymer mass during molding. No particular limitations exist on the basic product: filled, reinforced, self-extinguishing, and other materials can be used, except that great care should be given to handling and processing the granule, while steel fiber appearing on the surface of items produced in bright colors should be taken into account. The Latishields are used for molding business machine housings, containers for electronic devices (radio, telecommunications, defense and aeronautical systems, measuring equipment, electronic units for cars). In addition to the shielding effect, the Latishield s also feature good antistatic properties as well low resistivity which make them partially conductive.

Specific Notes for this Material: polycarbonate base (PC).

Disclaimer from LATI: This document contains information based on average values as obtained from the results of laboratory tests and observations made on LATI materials. Tested materials were injection molded, used in their natural color, and conditioned in compliance with Standard ASTM D 618, procedure A. These values refer to LATI's best technical and scientific knowledge at the moment of testing and cannot be used as a basis for the development of applications. For a better assessment of the materials, you are kindly requested to contact LATI's technical or commercial offices, which are at your disposal and will supply detailed information on the most suitable characteristics for their intended use. With reference to DPR n.224 dated May 24, 1988, issued in accordance with EC Guide-lines 85/374, LATI Industria Termoplastici S.p.A. declines all responsibility arising from an improper use of the products described in this document.

All data provided by LATI.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.24 g/cc0.0448 lb/in³ISO 1183
Linear Mold Shrinkage 0.0055 cm/cm0.0055 in/inLATI
Linear Mold Shrinkage, Transverse 0.0055 cm/cm0.0055 in/inLATI
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 63.0 MPa9140 psiISO 527
Flexural Modulus 2.60 GPa377 ksiASTM D790
Izod Impact, Notched 0.800 J/cm
@Temperature 23.0 °C
1.50 ft-lb/in
@Temperature 73.4 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 100 ohm100 ohmIEC 93
Comparative Tracking Index 85 V85 VIEC 112
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 138 °C280 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 - 280 °C500 - 536 °F
Mold Temperature 100 - 120 °C212 - 248 °F
Drying Temperature 120 - 130 °C248 - 266 °FNecessary, air ovens are sufficient. For thorough drying, use dehumidifiers or vacuum ovens. Avoid excessive working of the material.
Dry Time >= 3 hour>= 3 hour
 
Descriptive Properties
Injection Speedmedium - low

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Centro Plastica CiPiTENE® Recycled High Density Polyethylene Granules
Thermal Ceramics V-19 Block Insulation
Thermal Ceramics Therm-O-Seal Insulating Cements

PLATI208 / 50206

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.