MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Total PPH 4026 Polypropylene Homopolymer, Sheet Extrusion and Thermoforming
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Sheet/Thermoforming Grade

Material Notes: This grade belongs to the Total Ecosolution line.

Polypropylene PPH 4026 is a polypropylene homopolymer specifically developed to offer outstanding processability for sheet extrusion and thermoforming applications.

Polypropylene PPH 4026 is characterized by a higher stiffness than conventional nucleated homopolymers, a good impact resistance and an excellent clarity. Polypropylene PPH 4026 allows for wall thickness reduction while maintaining appropriate top load and crush resistances.

Polypropylene PPH 4026 has excellent organoleptic properties making it suitable for the most sensitive packaging application.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.905 g/cc0.905 g/ccISO 1183
Bulk Density 0.525 g/cc0.0190 lb/in³ISO 1183
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
3.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9595ISO 2039-2
Tensile Strength, Yield 39.0 MPa5660 psiISO 527-2
Elongation at Yield 9.0 %9.0 %ISO 527-2
Tensile Modulus 2.05 GPa297 ksiISO 527-2
Flexural Modulus 2.00 GPa290 ksiISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²2.38 ft-lb/in²ISO 180
Charpy Impact, Notched 0.600 J/cm²2.86 ft-lb/in²ISO 179
 
Thermal PropertiesMetricEnglishComments
Melting Point 163 °C325 °FISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 110 °C230 °F120°C per hour; ISO 752
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C140 °F120°C per hour; ISO 752
Vicat Softening Point  97.0 °C
@Load 5.10 kg
207 °F
@Load 11.2 lb
50°C per hour; ISO 306
 153 °C
@Load 1.02 kg
307 °F
@Load 2.25 lb
50°C per hour; ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total PPH 4026 Polypropylene Homopolymer, Film
Total PPH 4030 Polypropylene Homopolymer
ExxonMobil PP5341E1 Polypropylene Homopolymer
Total PPC 4252 Polypropylene, Impact Copolymer Corrugated Sheet
Total PPR 3260 Random Copolymer Polypropylene, Extrusion Grade

PTOTAL790 / 130515

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.