MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Total PPC 4252 Polypropylene, Impact Copolymer Corrugated Sheet
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Sheet/Thermoforming Grade

Material Notes: TOTAL Petrochemicals Polypropylene 4252 is a 1.5 melt flow rate impact copolymer designed for improved toughness and high melt strength. This resin offers outstanding processability in combination with excellent mechanical properties. Total polypropylene 4252 was specifically developed for the extruded cardboard market.

High Purity. Low catalyst residues in TOTAL Polypropylene 4252 allow extended processing runs without screen pack pluggage.

FDA. 4252 complies with all applicable FDA regulations for food contact applications

Recommended Applications. 4252 is recommended for corrugated sheet, profile extrusion, blow molding, thermoforming and slit film for carpet backing applications.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.905 g/cc0.905 g/ccASTM D1505
Melt Flow 1.5 g/10 min1.5 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 28.0 MPa4060 psiASTM D638
Elongation at Yield 6.5 %6.5 %ASTM D638
Flexural Modulus 1.25 GPa181 ksiASTM D790
Izod Impact, Notched 1.60 J/cm3.00 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 160 - 165 °C320 - 329 °FTOTAL Method
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C203 °FPressure unspecified; ASTM D648
 
Processing PropertiesMetricEnglishComments
Melt Temperature 204 - 260 °C400 - 500 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total PPC 4280W Polypropylene, Impact Copolymer
Total PPC 4481WZ Polypropylene, Impact Copolymer
Braskem TI4015F Impact Copolymer Polypropylene
Total PPH 4026 Polypropylene Homopolymer, Sheet Extrusion and Thermoforming
Total PPC 4170 Polypropylene, Impact Copolymer, Blown Film Grade

PTOTAL865 / 130590

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.