MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Total PPC 4280W Polypropylene, Impact Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: ATOFINA 4280W polypropylene is a nucleated impact copolymer. 4280W has a low fluidity providing melt strength with excellent impact properties. It is nucleated for added stiffness and surface hardness.

Application

ATOFINA 4280W is designed to be particularly suited for profile and sheet extrusion, extrusion-thermoforming and heavy-duty injection molded applications.

Information provided provided by Total Petrochemicals.

Total Petrochemicals acquired former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.905 g/cc0.0327 lb/in³ASTM D1505
Melt Flow 1.3 g/10 min1.3 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 24.8 MPa3600 psiASTM D638
Elongation at Yield 7.0 %7.0 %ASTM D638
Flexural Modulus 1.31 GPa190 ksiASTM D 790
Izod Impact, Notched NBNBASTM D256
 0.700 J/cm
@Temperature -20.0 °C
1.31 ft-lb/in
@Temperature -4.00 °F
ASTM D256
Charpy Impact Unnotched  0.800 J/cm²
@Temperature -20.0 °C
3.81 ft-lb/in²
@Temperature -4.00 °F
ASTM DIN53453
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ASTM DIN53453
 
Thermal PropertiesMetricEnglishComments
Melting Point 160 - 165 °C320 - 329 °FATOFINA Method
Deflection Temperature at 0.46 MPa (66 psi) 93.0 °C199 °FASTM D648
Vicat Softening Point 152 °C306 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total PPC 4252 Polypropylene, Impact Copolymer Corrugated Sheet
Total PPC 4481WZ Polypropylene, Impact Copolymer
Total PPC 4624WZ Polypropylene, Impact Copolymer
Total PPR 3221 Random Copolymer Polypropylene, Blow Molding and Sheet Extrusion
LyondellBasell Pro-fax SV152 Polypropylene Impact Copolymer

PFINAA065 / 38501

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.