MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

AISI 1330 Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Low Alloy Steel; Carbon Steel; AISI 1000 Series Steel; Low Carbon Steel

Material Notes: Applications for hot rolled bar include construction and machining into components; cold finished bar is suitable for heat treatment, machining into components, or constructional applications.

Key Words: UNS G13300, ASTM A322, ASTM A331, ASTM A519, MIL SPEC MIL-S-16974, SAE J404, SAE J440, SAE J770, DIN 1.1165, JIS SMn 1 H, JIS SCMn 2
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.87 g/cc0.284 lb/in³Typical for steel
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 179 - 335179 - 335average.
Hardness, Knoop 282282Converted from Brinell
Hardness, Rockwell B 9898Converted from Brinell
Hardness, Rockwell C 2525Converted from Brinell
Hardness, Vickers 271271Converted from Brinell
Modulus of Elasticity 200 GPa29000 ksiTypical for steel
Bulk Modulus 160 GPa23200 ksiTypical for steel
Poissons Ratio 0.290.29Typical For Steel
Machinability 55 %55 %Based on 100% machinability for AISI 1212 steel.
Shear Modulus 80.0 GPa11600 ksiTypical for steel
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000174 ohm-cm0.0000174 ohm-cmTypical steel
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.5 µm/m-°C
@Temperature 20.0 °C
6.39 µin/in-°F
@Temperature 68.0 °F
Typical steel
 12.2 µm/m-°C
@Temperature 0.000 - 300 °C
6.78 µin/in-°F
@Temperature 32.0 - 572 °F
Typical for steel
 13.9 µm/m-°C
@Temperature 0.000 - 500 °C
7.72 µin/in-°F
@Temperature 32.0 - 932 °F
Typical for steel
Specific Heat Capacity 0.472 J/g-°C0.113 BTU/lb-°FTypical steel
Thermal Conductivity 51.9 W/m-K360 BTU-in/hr-ft²-°FTypical steel
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.28 - 0.33 %0.28 - 0.33 %
Iron, Fe 97.35 - 97.97 %97.35 - 97.97 %As remainder
Manganese, Mn 1.6 - 1.9 %1.6 - 1.9 %
Phosphorus, P <= 0.035 %<= 0.035 %
Silicon, Si 0.15 - 0.35 %0.15 - 0.35 %
Sulfur, S <= 0.040 %<= 0.040 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Low Alloy Steel
AISI 1335 Steel
Overview of materials for AISI 4000 Series Steel
AISI 1330H Steel
AISI 1005 Steel

M1330A / 7317

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.