MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LG Chemical Lupox® PBT-HI1002F Impact Modified, Flame Retardant PBT Alloy
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: Flame Retardant, High Impact

Application: IT/OA, E&E (Switch)

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.33 g/cc0.0480 lb/in³ASTM D792
Water Absorption 0.080 %
@Time 86400 sec
0.080 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage 0.0090 - 0.013 cm/cm0.0090 - 0.013 in/inASTM D955
Melt Flow 4.0 g/10 min
@Load 2.16 kg,
Temperature 250 °C
4.0 g/10 min
@Load 4.76 lb,
Temperature 482 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 49.0 MPa
@Thickness 3.20 mm
7110 psi
@Thickness 0.126 in
50mm/min; ASTM D638
Elongation at Break 50 %
@Thickness 3.20 mm
50 %
@Thickness 0.126 in
50mm/min; ASTM D638
Flexural Strength 78.5 MPa
@Thickness 3.20 mm
11400 psi
@Thickness 0.126 in
1.3mm/min; ASTM D790
Flexural Modulus 1.96 GPa
@Thickness 3.20 mm
284 ksi
@Thickness 0.126 in
1.3mm/min; ASTM D790
Izod Impact, Notched 7.85 J/cm
@Thickness 3.20 mm
14.7 ft-lb/in
@Thickness 0.126 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Arc Resistance 120 - 179 sec120 - 179 secASTM D495
Comparative Tracking Index 250 - 399 V250 - 399 VSolution A; UL 746
 
Thermal PropertiesMetricEnglishComments
Melting Point 223 °C433 °FASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
@Thickness 3.20 mm
212 °F
@Thickness 0.126 in
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 100 °C
@Thickness 6.40 mm
212 °F
@Thickness 0.252 in
Unannealed; ASTM D648
UL RTI, Electrical 130 °C266 °FUL 746B
UL RTI, Mechanical with Impact 120 °C248 °FUL 746B
UL RTI, Mechanical without Impact 120 °C248 °FUL 746B
Flammability, UL94  V-0
@Thickness 0.750 mm
V-0
@Thickness 0.0295 in
 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 V-0
@Thickness 2.00 mm
V-0
@Thickness 0.0787 in
 V-0
@Thickness 2.30 mm
V-0
@Thickness 0.0906 in
 V-0
@Thickness 2.00 mm
V-0
@Thickness 0.0787 in
 5VA
@Thickness 2.30 mm
5VA
@Thickness 0.0906 in
 5VA
@Thickness 2.00 mm
5VA
@Thickness 0.0787 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 240 - 245 °C464 - 473 °F
Middle Barrel Temperature 245 - 250 °C473 - 482 °F
Front Barrel Temperature 250 - 255 °C482 - 491 °F
Nozzle Temperature 250 - 255 °C482 - 491 °F
Melt Temperature 250 - 265 °C482 - 509 °F
Mold Temperature 40.0 - 80.0 °C104 - 176 °F
Drying Temperature 100 - 120 °C
@Time 14400 - 21600 sec
212 - 248 °F
@Time 4.00 - 6.00 hour
Moisture Content <= 0.020 %<= 0.020 %
Shot Size 40 - 80 %40 - 80 %
Vent Depth 0.00254 - 0.00381 cm0.00100 - 0.00150 in
 
Descriptive Properties
Ram Speed SettingMedium to Fast
Screw SpeedMedium

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Bayblend® FR 110 Polycarbonate/ABS Blend
Chi Mei Polylac® PA-746Y ABS
Covestro Bayblend® FR 3010 Polycarbonate + ABS, Flame Retardant Grade
Covestro Bayblend® T65 HI PC/ABS Blend
Covestro Makrolon® 2405 MAS048 Polycarbonate

PLBA08f / 50366

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.