MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Master Bond EP101HTX-3 One Component Thermally Stable Epoxy System
Categories: Polymer; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: Master Bond EP101HTX-3 is a one component, high performance epoxy resin system with a long pot life at room temperature. It features high thermal stability, electrical insulation properties and excellent thermal shock resistance. EP101HTX-3 is suitable for coating, sealing, potting, encapsulation and impregnation applications.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Water Absorption  <= 0.50 %
@Temperature 23.9 °C,
Time 605000 sec
<= 0.50 %
@Temperature 75.0 °F,
Time 168 hour
Cured 3-5 hrs@ 250°F plus 5 hrs @ 300°F
 <= 0.50 %
@Temperature 23.9 °C,
Time 605000 sec
<= 0.50 %
@Temperature 75.0 °F,
Time 168 hour
Cured 8 hrs @ 300°F
Moisture Vapor Transmission  <= 22.7 cc-mm/m²-24hr-atm
@Temperature 40.0 °C
<= 57.6 cc-mil/100 in²-24hr-atm
@Temperature 104 °F
RH 95%, Cured 3-5 hrs@ 250°F plus 5 hrs @ 300°F
 <= 22.7 cc-mm/m²-24hr-atm
@Temperature 40.0 °C
<= 57.6 cc-mil/100 in²-24hr-atm
@Temperature 104 °F
RH 95%, Cured 8 hrs @ 300°F
Viscosity 1000 - 1500 cP
@Temperature 23.0 °C
1000 - 1500 cP
@Temperature 73.4 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 4141Cured 3-5 hrs@ 250°F plus 5 hrs @ 300°F
 4343Cured 8 hrs @ 300°F
Tensile Strength 80.0 MPa11600 psiCured 3-5 hrs@ 250°F plus 5 hrs @ 300°F
 83.4 MPa12100 psiCured 8 hrs @ 300°F
Elongation at Break 3.1 %3.1 %Cured 8 hrs @ 300°F
 3.4 %3.4 %Cured 3-5 hrs@ 250°F plus 5 hrs @ 300°F
Flexural Strength 119 MPa17200 psiCured 8 hrs @ 300°F
 121 MPa17500 psiCured 3-5 hrs@ 250°F plus 5 hrs @ 300°F
Compressive Strength 119 MPa17200 psiCured 8 hrs @ 300°F
 119 MPa17300 psiCured 3-5 hrs@ 250°F plus 5 hrs @ 300°F
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity  >= 1.00e+9 ohm-cm
@Temperature 200 °C
>= 1.00e+9 ohm-cm
@Temperature 392 °F
Cured 3-5 hrs@ 250°F plus 5 hrs @ 300°F
 >= 1.00e+10 ohm-cm
@Temperature 200 °C
>= 1.00e+10 ohm-cm
@Temperature 392 °F
Cured 8 hrs @ 300°F
 3.00e+11 ohm-cm
@Temperature 150 °C
3.00e+11 ohm-cm
@Temperature 302 °F
Cured 3-5 hrs@ 250°F plus 5 hrs @ 300°F
 3.60e+11 ohm-cm
@Temperature 150 °C
3.60e+11 ohm-cm
@Temperature 302 °F
Cured 8 hrs @ 300°F
 >= 3.00e+12 ohm-cm
@Temperature 100 °C
>= 3.00e+12 ohm-cm
@Temperature 212 °F
Cured 3-5 hrs@ 250°F plus 5 hrs @ 300°F
 >= 3.00e+12 ohm-cm
@Temperature 100 °C
>= 3.00e+12 ohm-cm
@Temperature 212 °F
Cured 8 hrs @ 300°F
 >= 2.00e+14 ohm-cm
@Temperature 25.0 °C
>= 2.00e+14 ohm-cm
@Temperature 77.0 °F
Cured 3-5 hrs@ 250°F plus 5 hrs @ 300°F
 >= 3.00e+14 ohm-cm
@Temperature 25.0 °C
>= 3.00e+14 ohm-cm
@Temperature 77.0 °F
Cured 8 hrs @ 300°F
Dielectric Constant  2.94
@Frequency 1e+6 Hz,
Temperature 100 °C
2.94
@Frequency 1e+6 Hz,
Temperature 212 °F
Cured 3-5 hrs@ 250°F plus 5 hrs @ 300°F
 2.99
@Frequency 1e+6 Hz,
Temperature 25.0 °C
2.99
@Frequency 1e+6 Hz,
Temperature 77.0 °F
Cured 3-5 hrs@ 250°F plus 5 hrs @ 300°F
 3.0
@Frequency 1000 Hz,
Temperature 100 °C
3.0
@Frequency 1000 Hz,
Temperature 212 °F
Cured 3-5 hrs@ 250°F plus 5 hrs @ 300°F
 3.01
@Frequency 1e+6 Hz,
Temperature 25.0 °C
3.01
@Frequency 1e+6 Hz,
Temperature 77.0 °F
Cured 8 hrs @ 300°F
 3.24
@Frequency 1000 Hz,
Temperature 25.0 °C
3.24
@Frequency 1000 Hz,
Temperature 77.0 °F
Cured 3-5 hrs@ 250°F plus 5 hrs @ 300°F
 3.25
@Frequency 60 Hz,
Temperature 25.0 °C
3.25
@Frequency 60 Hz,
Temperature 77.0 °F
Cured 8 hrs @ 300°F
 3.28
@Frequency 1000 Hz,
Temperature 150 °C
3.28
@Frequency 1000 Hz,
Temperature 302 °F
Cured 3-5 hrs@ 250°F plus 5 hrs @ 300°F
 3.28
@Frequency 1000 Hz,
Temperature 25.0 °C
3.28
@Frequency 1000 Hz,
Temperature 77.0 °F
Cured 8 hrs @ 300°F
 3.31
@Frequency 1e+6 Hz,
Temperature 150 °C
3.31
@Frequency 1e+6 Hz,
Temperature 302 °F
Cured 3-5 hrs@ 250°F plus 5 hrs @ 300°F
 3.34
@Frequency 60 Hz,
Temperature 25.0 °C
3.34
@Frequency 60 Hz,
Temperature 77.0 °F
Cured 3-5 hrs@ 250°F plus 5 hrs @ 300°F
 3.37
@Frequency 60 Hz,
Temperature 100 °C
3.37
@Frequency 60 Hz,
Temperature 212 °F
Cured 3-5 hrs@ 250°F plus 5 hrs @ 300°F
 3.38
@Frequency 60 Hz,
Temperature 100 °C
3.38
@Frequency 60 Hz,
Temperature 212 °F
Cured 8 hrs @ 300°F
 3.7
@Frequency 60 Hz,
Temperature 150 °C
3.7
@Frequency 60 Hz,
Temperature 302 °F
Cured 3-5 hrs@ 250°F plus 5 hrs @ 300°F
 3.74
@Frequency 60 Hz,
Temperature 150 °C
3.74
@Frequency 60 Hz,
Temperature 302 °F
Cured 8 hrs @ 300°F
Dissipation Factor  0.013
@Frequency 1e+6 Hz,
Temperature 100 °C
0.013
@Frequency 1e+6 Hz,
Temperature 212 °F
Cured 3-5 hrs@ 250°F plus 5 hrs @ 300°F
 0.013
@Frequency 1e+6 Hz,
Temperature 150 °C
0.013
@Frequency 1e+6 Hz,
Temperature 302 °F
Cured 3-5 hrs@ 250°F plus 5 hrs @ 300°F
 0.013
@Frequency 1e+6 Hz,
Temperature 150 °C
0.013
@Frequency 1e+6 Hz,
Temperature 302 °F
Cured 8 hrs @ 300°F
 0.014
@Frequency 1e+6 Hz,
Temperature 100 °C
0.014
@Frequency 1e+6 Hz,
Temperature 212 °F
Cured 8 hrs @ 300°F
 0.020
@Frequency 1e+6 Hz,
Temperature 25.0 °C
0.020
@Frequency 1e+6 Hz,
Temperature 77.0 °F
Cured 8 hrs @ 300°F
 0.021
@Frequency 1e+6 Hz,
Temperature 25.0 °C
0.021
@Frequency 1e+6 Hz,
Temperature 77.0 °F
Cured 3-5 hrs@ 250°F plus 5 hrs @ 300°F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 204 - 232 °C400 - 450 °Flong term
 246 - 260 °C475 - 500 °Fshort term
Minimum Service Temperature, Air -51.1 °C-60.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 120 - 360 min2.00 - 6.00 hourAt 250°F plus 6 to 10 hrs at 300°F
 
Descriptive Properties
Moisture vapor transmission<0.04 gm/ft2/24 hrs/inat 40°C, RH 95%, 3-5 hrs@ 250°F plus 5 hrs @ 300°F
 <0.04 gm/ft2/24 hrs/inat 40°C, RH 95%, 8 hrs @ 300°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Master Bond EP15 High Tensile Strength One Component Epoxy
Master Bond EP112 Two Component Epoxy
Master Bond EP76M Two Component, Nickel Filled Epoxy
Master Bond EP17HT-LO One component epoxy system for bonding, sealing, coating and casting

PMASTB266 / 132863

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.